Garment Inspection

It becomes necessary to maintain the quality right from the production stage in order to deliver a satisfactory final product to the consumer with the right quality which in turn results in getting continuous orders from the same customers. The garment manufacturers inspect their products by designated responsible inspectors then only the right quality product will reach the consumer. Under quality assurance process, the bulk production is inspected before delivered to the customers.

Previous Topic » Apparel Testing
Next Topic » Standard Apparel Construction Guidelines

Garment Inspection

All garment retailers expect to sell high quality products from manufactures. The quality of the garments any vary depends on the price market they are being made for so therefore buyers expect manufacturers expect manufacturers to follow various methods of inspection techniques all through the production and prior to shipment release from factory. Following correct inspection procedures, inspection systems and eventually shipment release gives the clear judgment of the quality of the garment.

Under quality assurance process, the bulk production is inspected before delivery to the customer to examine if it meets the specifications. The consumers want to get quality products and the products should reach the consumers with right quality.

Quality assurance covers all the processes within a factory that contributes to the production of quality garment products and is conducted right from where housing, manufacturing, finishing and packing process until shipment is released. The final inspection is carved out by buyer representative or independent auditors free from any pressure from vendor or factory representative. Air of final inspection is to visually inspect articles at random from fully or 80-90% packed purchase order to verify their general conformity and appearance with instruction/description and/or reference tagged sample received from buyer. Result is documented and recorded as reference but still vendor/manufacturer is always responsible for claims if any arising due to any defective goods found packed and inspected at buyers warehouse.

  

Types of Inspections

Pre-Production Inspection: This is done before production starts. It is done to crosscheck for final verification of Bulk fabric and trims materials, styling cutting way, manufacturing details and workmanship of the garment or pre-production sample as per the customer requirement.

1st inline production inspection: This inspection is done at the start of production when first production output of particular style of garments is inspected; to distinguish possible discrepancies or variation and to do necessary corrections to be made bulk production. This type of inspection is done at preliminary stage of manufacturing of a style covering mainly style detail, general appearance, workmanship, measurements, fabric quality, Trims and components, Lot color, printing, embellishments and washing quality.

2nd line Production Inspection: This inspection is done during production to ensure initial discrepancies have been corrected and rectified. This inspection is a follow-up of the 1 st inline production inspection and is generally carried out after 1st line inspection when discrepancies have been detected at that time.

Final Random Inspection: This inspection is carried out when the production of the total quantity of an order or partial delivery is completed. A sample lot will be selected from the order and a percentage of the garments will be inspected, this percentage usually being stipulated by the buyer. The AQL sampling inspection system as specified by the buyer.

  

Garment Defects Classification

Once the samples are selected, each article is to be individually inspected. Defects detected during an inspection are buyer specific so therefore vary from one buyer to another. Defects are classified within the following categories:

  • Critical Defect: A serious defect that can cause harm or injury to the user and/or result in a hazardous condition.
  • Major defects: A defect that falls to meet the mandatory regulations directly affecting the usability, salability, safety and value of the merchandise or as specified by customer buyer are considered as major defects and are generally non repairable for example fabric hole, shading among panel, wrong measurement, foreign yarn, dye patches etc. The measurement tolerate level may vary from customer to customer.
  • Minor Defects: A defect that does not adversely affect the usability of the product but does consists of a deviation from the original sample, and may affect the sale of the product. Some of these defects are due to workmanship and some can be repairable but still can deteriorate the serviceability of the merchandise for example stain, skip stitch, wavy bottom hem etc.
  

AQL Random Sampling inspection

AQL stands for Acceptable Quality level. The AQL determines the maximum amount of admitted defective units in a sample. AQL, for purposes of sampling inspection, can be considered satisfactory as a process average. The most commonly used AQL is a major 2.5 Minor 4.0. The AQL random sampling inspection is derived from the mathematical theory of probability and is based on the sampling these defined in military standard 105D (MIL - STD - 105D). Some defectives are considered acceptable.

This method constitutes taking random sample from a lot of merchandise, inspecting them and depending on the quality of the sample inspected determining whether the entire lot is acceptable or not. The MIS - STD - 105D (also BS 6001, ISO 2859, DIN 40080) provides the sampling plans; and these determine the number of samples of be inspected in lot size, in addition to indicating and the acceptable quality level (AQL) which represents the maximum number of defects per hundred units that, for the purpose of the sampling inspection can be considered satisfactory as a process average.

In general cases the buyer will determine which sampling plan and what AQL to adopt. The AQL 1.5 is applied when severe inspection conditions are required for expensive items like up market or Boutiques. The AQL 2.5 is applied when textiles or normal/good quality are involved. There are three types of sampling plans. Each sampling plan can be performed at three levels, i.e. normal tightened and reduced, depending on inspection requirements and quality of the products. In the garments industry generally single and double normal sampling plans are applied. The sample size code letter table shows various lot sizes corresponding to a series of code letters. There are seven inspection levels, four for general inspection (already mentioned) and three for special inspection. For garment inspection, general inspection level II (normal II) is normally applied.

  

Inspection Methods

Single sampling plan - Normal inspection

Assurance as AQL 2.5% and a lot of 1,200 garments and the sample size is 80 garments. If the number of defective garments found are 5 the total lot is "Acceptable" suppose if the garments found is 6, the total lot is "Reject/Re-Check".

Double sampling plan - normal inspection

Assurance an AQL 4.0% and lot size is 1,200 garments and the sample size is 80 garments. If the number of defective garments found is 7, the total lot is "Acceptable" suppose if the defective garments found are 8, the total lot is "Reject/Re-check". Today most of the customer demand for high quality products in low prices. So we should maintain the quality from the beginning stage of the production then only the final product with reach the consumer with right quality and we can get the order continuously from our customers. The garment manufacturers inspect their products continuously by designated responsible inspectors then only the right quality product will reach the consumers.

  

Inspection-shipment carton selection

For pre-final inspection, selection of cartons from total cartons packed can be done based as shown table:

No. Total cartons in Shipment Carton Selected
1 1-15" 2
2 15-25 3
3 26-90 5
4 91-150 8
5 151-280 13
6 281-500 20
7 501 and above 32
  
« Previous Topic
Apparel Testing
Next Topic »
Standard Apparel Construction Guidelines
Testing is a valuable aid for textile production, distribution, and consumption. During textiles testing the variation of a fibre or fabric i.e. length, colour, fineness, threads per inch, cover factor, is detected properly. Continuous test of the textiles results a enhanced and efficient output of the production. By Apparel Testing we can evaluate and ensure the quality of the garments to be used by the end users.Description-The standards specified are minimum standards, and provide guidelines for apparel construction and performance to achieve consumer satisfaction.This knowledge will be helpful for buyers, suppliers and Agents.The standards objective is to deliver quality merchandise to the customer. It applies to all categories of apparel and textiles.