Tenacity Conversions (Free Strength) g = gms
| |
g/den |
g/tex |
g/dtex |
cN/tex |
| g/den |
1 |
( g/tex ) / 9 |
( g/dtex ) x 10 / 9 |
( cN/tex ) x 0.113 |
| g/tex |
( g/den ) x 9 |
1 |
( g/dtex ) x 10 |
( cN/tex ) x 1.02 |
| g/dtex |
( g/den ) x 0.9 |
( g/tex ) / 10 |
1 |
( cN/tex ) x 0.102 |
| cN/tex |
( g/den ) / 0.113 |
( g/tex ) / 1.02 |
( g/dtex ) / 0.102 |
1 |