Consumers should be aware of several cautions in relation to proper use and care of fabrics made from rayon fiber. Regular or viscose rayon has low wet strength, resulting in loss of stability or the tendency to shrink or stretch easily when wet. Although resin-treated rayons can sometimes be hand or machine washed with success, regular rayon normally requires dry cleaning to maintain appearance and shape.
There is a finish that can be applied to make viscose rayon fabrics washable and limit shrinkage to 3 percent. It is formaldehyde-free and will not affect the hand, width, or length of treated fabrics. It can be used on challis,failles, and other fabrics that otherwise would require dry cleaning to maintain appearance.
Consumers should also note that HWM or polynosic rayon has high wet strength. Fabrics made from this fiber can usually be machine washed and tumble dried. Polynosic rayon functions and handles during use and care similarly to cotton. Unfortunately, it is often difficult to identify whether a garment is made from polynosic or viscose rayon unless identified on the label. Read labels, look for trade names, and follow care recommendations.
In some instances, polynosic or HWM rayons may be “low labeled.” This means that manufacturers have recommended dry cleaning when hand washing or machine washing would be satisfactory. Sometimes the fabric may be washable, but trims, linings, or other aspects of the garment may not be. Unfortunately, consumers take a risk when they care for a rayon garment in a manner other than that recommended by the care label.
Moisture-Sensitive Sizing and Dyes—Sizings or starches applied to rayon during finishing give body, sheen, lustre, shape, and control relaxation shrinkage. In some instances, they may enhance strength. Unfortunately, some of the sizings and dyes used on rayon are sensitive to moisture. When moisture contacts them, the sizing or dye migrates to the edge of the wet spot, and forms a “ring” on the fabric. Rain drops, splashes from tap water, as well as water-based food substances will form dark rings on these fabrics. The rings may be difficult to remove without submerging the entire garment in water. This process can cause further damage to viscose rayons, which have low wet strength.
The migration of dyes and sizings from moisture further complicates stain removal in dry cleaned garments. Dry cleaning solvents are designed to remove oil-based stains. Water-based stains such as fruit juice and beverages, and certain foodstuffs require moisture for stain removal. While this process removes the stain, it may also cause dye or sizing migration in the rayon fabrics, leaving a water spot ring. Also, as a result of the general dry cleaning process, swirls or waves may occur on the fabric surface. This is caused by a disturbance in the sizing from moisture in steam pressing, compounded by heat and pressure associated with the process. Generally these surface disturbances cannot be completely removed.
Loss of Body—Rayon fabrics may lose body or become limp over time from abrasion or general removal of sizing during dry cleaning. Dry cleaners can apply sizings, but they seldom duplicate the effect achieved during commercial processing. Application of sizing also reduces seam slippage, ravelling, and fraying of fabrics.
Since the finish is not permanent, it can result in changes in fabrics and their performance, such as loss of body, lustre, seam slippage, and ravelling. The consumer should note that moisture-sensitive dyes or finishes are generally not applied to polynosic rayons and should not cause problems during use and care of these fabrics.
Also related to sizing application is yellowing of fabrics over time. Some sizings or starches oxidize and yellow with age. The problem is most noticeable on exposed areas such as collars, shoulders, and outside sleeves, especially on white or light-colored fabrics. Wet cleaning, often accompanied by bleaching will correct the problem; however, this treatment may cause additional damage from shrinkage or loss of body.
Other cautions related to rayons are pilling, relaxation shrinkage, and fusing of blends. Short, low-twist fibers, which contribute a soft hand to garments, rub or abrade during wear. These fibers mat together and form fiber balls or pills on the fabric surface. Pills may be “shaved” or clipped off; however, as this is done, fibers are being removed, creating a thinner layer of fabric. The problem is less likely to occur on fabrics with a hard surface and those made from longer, or higher twist yarns.
Rayon fabric is especially susceptible to relaxation shrinkage, which occurs over a period of time from routine laundering or dry cleaning. Consumers should consider this tendency when selecting garments, particularly those that are more fitted.
Because viscose rayon is less stable when wet, uneven hemlines may occur in full bias skirts or dresses made from rayon crepe fabrics. The problem can be especially bothersome in damp climates. Bias hemlines are notorious for stretching and changing length over time, but especially so if garments are made from viscose rayon crepe. Hems in these garments may need to be re-marked and evened-up over time.
Rayon is a versatile fiber and is frequently found in blends with polyester, nylon, and acrylic—all of which are synthetics and heat sensitive. These fibers generally contribute strength, wrinkle resistance, and ease of care to rayon blends. During care, iron temperatures safe for rayon can be too hot, melting or fusing the heat-sensitive synthetic fibers. This process cannot be reversed and results in slits, tears, brittleness in the fabric, or shiny areas.