Cotton Fibres - the king of fibres

Cotton is a soft staple fibre that grown in a form known as a boll around the seeds of the cotton plant, a shrub native to tropical and subtropical regions.

Previous Topic » Natural Cellulosic Seed Fibres
Next Topic » Cotton Fibers and Its Properties

Cotton

cotton boll

Cotton today is the most used textile fiber in the world. Its current market share is 56 percent for all fibers used for apparel and home furnishings and sold in the U.S. Another contribution is attributed to nonwoven textiles and personal care items. The earliest evidence of using cotton is from India and the date assigned to this fabric is 3000 B.C. There were also excavations of cotton fabrics of comparable age in Southern America. Cotton cultivation first spread from India to Egypt, China and the South Pacific.

Cotton is a soft, staple fiber that grows in a form known as a boll around the seeds of the cotton plant, a shrub native to tropical and subtropical regions around the world, including the Americas, India and Africa. The fiber most often is spun into yarn or thread and used to make a soft, breathable textile, which is the most widely used natural-fiber cloth in clothing today. The English name derives from the Arabic (al) qutn قُطْن , which began to be used circa 1400.

Each cotton fiber is composed of concentric layers. The cuticle layer on the fiber itself is separable from the fiber and consists of wax and pectin materials.

  

Properties of Cotton

cotton boll

Cotton is a soft fibre that grows around the seeds of the cotton plant. Cotton fibre grows in the seed pod or boll of the cotton plant. Each fibre is a single elongated cell that is flat twisted and ribbon like with a wide inner hollow (lumen).

  • 90% cellulose, 6% moisture and the remainder fats and impurities
  • The outer surface is covered with a protective wax like coating which gives fibre an adhesive quality

Cotton is a natural fiber that is grown in countries around the world. It is a crop that requires adequate moisture and heat to mature and produce quality fibers. Cotton growing tends to be in warmer climates. Cotton is a true commodity in the world markets and supply and demand truly affect prices of raw cotton.

Cotton fibers are mainly made up of cellulose. Cellulose does not form unless temperatures are over 70 °F (21 °C). The cotton fibers are attached to the seeds inside the boll of the plant. There are usually six or seven seeds in a boll and up to 20,000 f ibers attached to each seed. The length of these fibers (also called staples) is the main determining factor in the quality of the cotton. In general, the longer the staple grows the higher the quality of the cotton. Staple lengths are divided into short, medium, and long (and extra long, in some cases):

  • Short staple cotton is between 3/8” to 15/16” (.95cm to 2.4cm) in length
  • Medium staple cotton is between 1” to 1-1/8” (2.54cm to 2.86cm) in length
  • Long staple cotton is between 1-3/16” to 2-1/2” (3cm to 6.35cm) in length

Properties of Cotton Products

  • Comfortable – there are no surface characteristics of cotton that make it irritating to human skin. Cotton feels good against skin; it has a soft hand.
  • Hydrophilic – cotton has a natural affinity for water – it attracts moisture away from your body.
  • Moisture passes freely through cotton – aiding in evaporation and cooling
  • Good Heat Conductivity – Cotton allows heat to dissipate making it a wonderful fiber to maintain a comfortable sleeping temperature.
  • Strong and abrasion resistance
  • The unfavorable attributes of cotton include its lack of resiliency (cotton tends to wrinkle) and its lack of luster (colors are usually dull).

Properties of Cotton Fiber

  • It has 8% moisture regain
  • The cellulose is arranged in a way that gives cotton unique properties of strength, durability, and absorbency
  • It is fresh, crisp, comfortable, absorbent, flexible, has no pilling problems and has good resistance to alkalis
  • It has poor wrinkle resistance, shrinkage, poor acid resistance, less abrasion resistance, susceptible to damage by moths and mildew, needs lots of maintenance and stains are difficult to remove
  • Its fibre length ranges from ½ inches to 2inches
  • It has 10%increase in strength when wet.
  • It has a flat twisted tube shap

Long Staple Cotton

In general, long staple cottons are needed to spin the yarns needed in the weaving of the finer down proof cotton fabrics.

Long staple cottons are considered to be finer quality because they can be spun into finer yarns and those finer yarns can be woven in to softer, smoother, stronger, and more lustrous fabrics. Long staple cottons make stronger yarns, especially in fine yarns, as there are less fibers in a given length of yarn and the longer fibers provide more points of contact between the fibers when they are twisted together in the spinning process. Common areas that grow long staple cottons in the world would be Egypt, Sudan, the United States (Pima cottons grown in the west and southwest are long staple cottons), and Western China. The two most widely known long staple cottons are Egyptian cotton and Pima cotton. Pima cottons are grown mainly in the United States, but also in Peru, Israel, and Australia.

The fibers are sent to a textile mill where carding machines turn the fibers into cotton yarn. The yarns are woven into cloth that is comfortable and easy to wash but does wrinkle easily. Cotton fabric will shrink about 3% when washed unless pre-treated to resist shrinking.

Cotton is prized for its comfort, easy care, and affordability and is ideal for clothing, bedding, towels, and furnishings.

  

Classing Cotton

Cotton buyers judge cotton on the basis of samples cut from the bales. Skilled cotton classers grade or "class" the cotton according to standards established by the US Department of Agriculture such as cleanliness, degree of whiteness, length of fiber, and fiber strength.

The classers pull a sample. They discard most of the cotton until just a pinch of well-aligned fibers remains. They measure the length of the fibers, referred to as staple fibers. Longer staple fibers are higher-grade cotton and are sold at higher prices. Long staples range from 1.1 inches to 1.4 inches long.

  

Harvesting

cotton stipper machineCotton was once harvested by hand, often by slave labor or tenant farmers. As recently as 1965, over a fourth of the U.S. cotton crop was picked by hand. Today, harvesting cotton is highly mechanized.

Harvesting machines called strippers and pickers efficiently remove the cotton, while leaving the plants undisturbed. Spindle harvester, also called a picker, has drums with spindles that pull the cotton from the boll in one or two rows at a time. Even a one row mechanical picker can do the work formerly done by 40 hand pickers.

In stripper harvesting, the stripper moves along rows of plants, passing them between revolving rollers or brushes that pull off the cotton. Strippers also pull twigs and leaves with the cotton.

Cotton gins separate the fibers, called lint, from the seeds. After ginning, the cotton goes to the bale press that packs it into 480 pound bales about the size of a large refrigerator.

  

Cotton Ginning

cotton baleFrom the field, seed cotton moves to nearby gins for separation of lint and seed. The cotton first goes through dryers to reduce moisture content and then through cleaning equipment to remove foreign matter. These operations facilitate processing and improve fiber quality. The cotton is then air conveyed to gin stands where revolving circular saws pull the lint through closely spaced ribs that prevent the seed from passing through. The lint is removed from the saw teeth by air blasts or rotating brushes, and then compressed into bales weighing approximately 500 pounds. Cotton is then moved to a warehouse for storage until it is shipped to a textile mill for use.

A typical gin will process about 12 bales per hour, while some of today’s more modern gins may process as many as 60 bales an hour.

Ginning Process diagram
  

Ginning Process Flowchart

Ginning Process Flowchart
  

Inside the Cotton Gin - Video

  

Cellulose is the substance that makes up most of a plant's cell walls. Since it is made by all plants, it is probably the most abundant organic compound on Earth.Many varieties of plant fibres exist such as hairs (cotton, kapok), fibre-sheafs of dicoltylic plants or vessel-sheafs of monocotylic plants (e.g. flax, hemp, jute and ramie), and hard fibres (sisal,henequen and coir), not to mention the large number of fibres obtained from trees. Byproducts of agricultural crops are being considered as

Kapok/Capok fibre is one of the natural cellulosic fibres which grow on the kapok plant. It has a hollow body and a sealed tail, which are desirable features of candidates for functional textiles of this nature. However, the low volume weight of kapok is (specific density 0.29g/cm3), and the short length and smooth surface of the fibres, causing poor inter-fibre cohesion, have prevented kapok from being processed by modern spinning machines.