Contains the process sequence of Finishing for yarn. It includes yarn twist setting, cone winding from ring cops to cone by cone winding , ordinary cone winding specifications, slub catcher settings , splicing, production calculation.

0 985

Yarn Finishing System

Yarn finishing starts after Ring Till transfer to finished godown.

Selling of yarn: Yarn is sold in a) hank form b) Cone form.

Slub Catcher setting:

Lower the count, higher the slub catcher setting gap. Slub catcher should keep clean, otherwise, fluff will accumulate.

Splicing-Piecing of yarn without knotting.Done by compressor sir, Manual knotting also can be done.

Production calculation

Prod/shift in kg/m/c =Speed of Drum (rpm)*3.14()*Die of Drum (inch)*60*8*efficiency*No. of Drum
 36*840*Count of yarn

The process sequence of Finishing

Process sequence of finishing

Yarn Twist Setting:

Object: To improve the resistance of the yarn to untwisting and snarling, it is necessary to fix to twist i.e. to bring the yarn into a stabilized state.

Bad/methods mostly used

  • Yarn steaming in an autoclave (with boiler) capacity up to 500 kg/batch. Allowable pressure 7kg/cm(max)
  • High-frequency current by the electrode with high voltage
  • Water treatment conditioning

Cone Winding

From Ring cops to cone by cone winding, ordinary cone winding specifications

  • No. drum/m/c—120
  • Drum Dia—80-95 mm
  • Traverse—150mm-152mm
  • Type of package shape—9 degrees 15
  • Winding speed—500-850m/tm
  • Ribbon breaking device: Electrical on-off type
  • Empty bobbin conveyor at each side with an endless belt
  • Provision for a rack on the top goes m/c for storing ring cops.
  • Stop motion—Auto stop for end breakage with individual spindle control
  • Main motor—each side of the individual motor
  • The speed of winding drum—up to—3500 rpm
  • Overhead blower—for cleaning fly
  • Suction arrangement for slub catcher
  • Splicing device
  • Type of package- Paper or plastic

Leave A Reply

Your email address will not be published.

This site uses Akismet to reduce spam. Learn how your comment data is processed.

This website uses cookies to improve your experience. We'll assume you're ok with this, but you can opt-out if you wish. AcceptRead More