Characteristics of Rayon Fiber

Rayon is moisture absorbent (more so than cotton), breathable, comfortable to wear, and easily dyed in vivid colors. It does not build up static electricity, nor will it pill unless the fabric is made from short, low-twist yarns.

Rayon Fiber – the Multi-Faceted Fiber

Of all the fibers, rayon is probably the most perplexing to consumers. It can be found in cotton-like end uses, as well as sumptuous velvets and taffetas. It may function successfully in absorbent hygiene and incontinence pads and equally well-providing strength in tire cords.

Basics of Rayon Fiber

Rayon is often used in fashion and home furnishings, but the fiber is also found in sanitary products, diapers, and medical supplies.

Manmade Regenerated Cellulose Fibers

Certain natural cellulose fibers are treated and re-produced for specific purposes. The famous fibers such as Viscose Rayon, Acetate etc. are produced by processing various natural polymers.