Yarn Spinning & Preparation
CSP lets you compare strength across counts. Always quote it with the target it is being judged against.
—
Lea strength in pounds x English count
CSP depends on the tester, humidity and skein preparation. Compare only figures produced under the same standard atmosphere of 20C and 65% RH.
Count Strength Product (CSP) Calculator — free, with the formula and a worked example, at Textile School.