Fabric Relaxation Shrinkage Calculator

Mass is conserved while area contracts, so a shrinking knit always gets heavier.

Length Direction Marked before and after
cm
cm
Width Direction Marked before and after
cm
cm
Fabric Before relaxation
g/m²

Length Shrinkage

— %

Positive values mean the fabric contracted

Dimensional Change

Width Shrinkage
— %
Area Shrinkage
— %
Weight Gain
— %
Relaxed Fabric GSM
— g/m²

Follow the reference relaxation procedure the buyer specifies. Dry relaxation, wet relaxation and full tumble relaxation give three different numbers on the same fabric.

Fabric Relaxation Shrinkage Calculator — free, with the formula and a worked example, at Textile School.