Tire Cord Dipped vs Greige Contraction Calculator

The dipping unit shortens, narrows, densifies and adds weight in one pass. Design the greige for what leaves the dip, not what enters it.

Dimensions Before and after
m
m
cm
cm
Construction Greige
epi
g/m²
%

Length Contraction

— %

Machine-direction shrinkage through the dipping unit

Dipped Fabric

Width Contraction
— %
Area Contraction
— %
Dipped Ends per Inch
— epi
Dipped Areal Weight
— g/m²
RFL Solids Added
— g/m²

Contraction depends on the tension held through the dip and cure zones, so a fabric run at a different stretch setting will not reproduce these figures. Tire reinforcement is a safety-critical application — treat this as construction planning and confirm dipped dimensions and adhesion on the actual line.

Tire Cord Dipped vs Greige Contraction Calculator — free, with the formula and a worked example, at Textile School.