Draw frame Functions

Carded Slivers are fed into the Draw-Frame and are stretched/Straightened and made into a single sliver. Also, fibre blending can be done at this stage. The cans that contain the sliver are placed along the draw-frame feeder rack, usually…

Yarn Spinning, Blow Room Functions

Blow room is the starting of the spinning operation where the fiber is opened, cleaned, mixed, micro dust removed and evened thus passed to carding machine without increasing fiber rupture, fiber neps, broken seed particles and without…

Functions of Carding Machine

Carding is a mechanical process that breaks up locks and unorganized clumps of fiber and then aligns the individual fibers so that they are more or less parallel with each other. Carding can also be used to create blends of different fibers…

Staple Yarn Spinning

The larger part of staple fibre, approx. 33 mio tons are processed in short staple spinning. This part of the spinning industry therefore is of great significance in the world of textile production.

Yarn Formation/Spinning

The Fibre formation process includes a change in shape, structure, and properties of the thermoplastic polymer. The polymer pellets or granules are fed into an extruder where, through heating, their melting temperature is exceeded. The…

Yarn Spinning – Formation of Yarn

Yarn spinning is the process of manufacturing yarn from different types of fibres into a continuous length from one or more type of fibers. Spinning is the most important and the initial step in fabric manufacturing. The major goals of…