Polymer Fibres

Polymers are made up of many molecules all strung together to form really long chains. Things that are made of polymers look, feel, and act depending on how their atoms and molecules are connected.

Manmade Protein Fibers

Manmade protein fibers are produced by dissolving proteins like casein from milk, soya bean protein, and zein from corn in diluted alkali and forcing these solutions through a spinneret into an acid-formaldehyde coagulating bath.

Synthetic Fibers

The synthetic man-made fibers include the polyamides (nylon), polyesters, acrylics, polyolefin, vinyl, and elastomeric fibers, while the regenerated fibers include rayon, the cellulose acetates, the regenerated proteins, glass and rubber…

Man-made /Artificial fibers

Man-made fibers are fibers in which either the basic chemical units have been formed by chemical synthesis followed by fiber formation or the polymers from natural sources have been dissolved and regenerated after passage through a…

Natural Protein Fibres

The protein fibers are formed by natural animal sources through condensation of a-amino acids to form repeating polyamide units with a various substituent on the a-carbon atom. In general, protein fibers are fibers of moderate strength,…