The two major categories based on the types of weaves are Basic or Simple weave and Compound or complex weaves which are further categorized into the following categories:
Basic/Simple Weaves
- Plain Weave
- Twill Weave
- Satin Weave
Compound/Complex/Novelty Weaves
- Dobby Weave
- Jacquard Weave
- Double Cloth & Double Weave
- Pique
- Pile Fabrics
- Surface Figure Weaves
Basic/Simple Weaves
-
Plain Weave
Simplest weave requiring a 2 harness loom, formed by yarns at right angles whereby each warp yarn interlaces with each weft yarn Properties: least expensive to produce, reversible unless surface design, wrinkles more, firm & wears well, less absorbent, abrasion resistant, used as background for printing/ embroidery
- Rib Weave fabrics: Rib effect is produced by using heavy yarns in the filling direction or by more warp than
filling yarns per inch. Eg Bengaline, ottoman, faille, poplin, broadcloth, taffeta. - Basket Weave fabrics: Basketweave is made by treating two or more yarns as one in either the warp or weft or
both the directions and interlacing them in plain weave. It is not as firm as plain weave, have more yarn slippage, shrinks easily. Eg 2X1, 2X2, 2X4, 3X2, 4X4. Oxford cloth is 2X1 & monk cloth is 4X4. Flat duck, hopsacking, Panama are other examples.
- Rib Weave fabrics: Rib effect is produced by using heavy yarns in the filling direction or by more warp than
-
Twill Weave
Each warp or weft yarn floats across two or more weft or warp yarns with a progression of interlacing by one to the right or to the left, forming a distinct diagonal line or wale.
The direction of diagonal may be formed from right to left, from left to right or a combination of both. Soil resistant, softer & pliable, good wrinkle recovery, durable & wears well. The direction of the twill on the back of the cloth is opposite to the twill line on the face. 3 harness is required for twill weave.- Right Hand Twill – diagonals run upwards to the right
- Left Hand Twill – diagonals run upwards to the left.
- Balanced Twill – the same number of warp pass over filling yarns. It is reversible. 2X2, 4X4
- Unbalanced Twill – have an uneven warp or filling yarn. It has a right or wrong.
- Broken Twill – combines right or left-hand twills
- Herringbone Twill – a series of inverted V’s are formed resembling the backbone of the
herringbone fish. Most commonly used in suiting fabrics. - Twill Angles – according to the angles of the diagonal line, Regular twill – 45° °
- Reclining twill – with smaller angles, Steep twill – with larger angles. E.g.: denim, herringbone, houndstooth
-
Satin Weave
Each warp/ filling yarn floats over 4 filling/ warp yarns & interlaces with 5th filling/ warp yarn, with a progression of interlacing by 2 to right or left (warp-faced/ weft faced). Luster (long floats), firm, durable (yarns packed closely together), pliable, wrinkle resistant,
yarn slippage. Satin is warp faced. Sateen is weft-faced. 5 harness is required for a satin
weave.
Compound/Complex/Novelty Weaves/ Figure/ Decorative weave
-
Dobby Weave
Small figured designs (floral or geometrical) woven repeatedly throughout the fabric,
produced by a combination of two or more basic weaves, using a dobby attachment on
the loom. Weaving pattern controlled by a plastic tape with punched holes that control
the raising & lowering of warp yarns. It uses up to 32 harnesses. -
Jacquard Weave
Characteristics: highly intricate large designs using colored yarns and multi-weaves
produced on a loom with jacquard attachment. Incorporates all 3 basic weaves & their
combination. Each warp yarn is controlled separately by punched cards that are laced
together in a continuous strip. Are more expensive. Used for home furnishing, apparel,
elaborate & decorative fabrics. Eg Brocade, Damask, tapestry, brocatelle, matelasse -
Surface Figure /Extra Yarn Weaves
Extra warp or weft yarn introduced in fabric to produce designs at regular intervals.
Between 2 motifs, extra yarn floats across the back of the fabric.- Clipped / unclipped Spot – embroidery-like design is achieved through either extra warp or weft yarn. Long floats on the back when a cut is called Clipped Spot & when
uncut – Unclipped Spot. - Swivel – contains extra filling yarns. In this weave, the extra yarn is interlaced with the
background at different places to avoid pulling. These are stronger than Spot
weave. - Lappet – contains extra warp yarns.
- Clipped / unclipped Spot – embroidery-like design is achieved through either extra warp or weft yarn. Long floats on the back when a cut is called Clipped Spot & when
-
Pique
Lightweight to heavyweight cotton fabric with a raised woven design. Lengthwise wales
or cords on the face of fabric (formed by extra warp yarns) that are held in place by
crosswise weft floats on the back of the fabric. Extra warp yarns (stuffer yarns) do not show on the face of the fabric. They are not interwoven but laid under the cords to emphasize the quilted effect. Made of dobby or jacquard loom. Eg waffle, huck toweling, granite, honeycomb, bedcord, pique -
Double Cloth
They are made with 3, 4 or 5 sets of yarn. Two fabrics are woven together on the same
loom, one above the other & laced together with an extra set of warp or weft yarns called
binder yarns (5 sets of yarns). Pile fabrics are commonly prepared by this method.
Produces a variety of fabrics, reversible, stable, may have different color or design on the
two sides. Used for upholstery, drapery, and heavy apparels.
Other Special Weaves
-
Crepe Weave
Crinkled or pebbly surface. Irregular, indistinct pattern utilizing both plain and satin
weave using dobby attachment are made. Few crepe weave fabric is available.
Other crepe fabrics are created using crepe yarn which is highly twisted (up to 65 tpi).
Textured yarns, bicomponent yarns (uneven shrinkage), embossing, stamping crepe like
effect are being used. In all these plain weaves, synthetic fibers and thermoplastic property
are used. -
Leno Weave
It is the form of weaving in which two adjacent warp yarns cross each other between the picks. The warp yarns are paired. With a special leno or doup, attachment warp yarns are crossed/ twisted over each other in pairs around each pick, firmly holding the filling yarn
in the figure – 8 loops formed. Leno fabrics are open and gauge like. Leno weave is
useful in reducing yarn slippage, greater firmness & strength than plain weave. Uses-
curtain, gauge, marquisette, grenadine, fruit sacks, rice net, mosquito net, mesh. -
Colour & Weave Effect
A pattern produced in a fabric by using a certain weave and a certain arrangement of
differently colored yarns in both warp and filling.Hound’s tooth – 2 up, 2 down, 45° left-hand twill, and a group of 4 yarns of one color are
arranged in both warp & filling followed by the other color. -
Lappet weave
This is the type of weave in which floating threads are carried on the surface of the fabric and introduced at intervals to form the patterns. The floats are not long and the patterns are usually geometric, i.e. zigzag stripes in white yarn on a colored plain weave ground.
-
Novelty weave
Any weave which varies or combines the basic weaves, plain, satin and twill.
-
Swivel weaving
A fabric in which figure is achieved by the introduction of additional weft threads into base fabric to produce small clipped woven-in-spot effects. The figuring yarn is fed from a series of shuttles mounted over the top of the weaving surface.
-
Tablet Weaving
It is a method of making woven plain or patterned narrow fabrics, where the warp is controlled by tablets made of thin, stiff material, e.g. cardboard, plastic, bone, etc. Tablets are usually about 5 to 10 cm square, although other shapes, e.g. triangles, hexagons, etc. are also used. Each tablet has a hole at each corner through the warp yarns are threaded. Rotating the tablets controls the rise and fall of the warp yarns.
-
Woven Pile Fabrics
3-dimensional fabrics, utilizing 3 sets of yarns, warp & weft to form base fabric & extra
set of warp or weft yarns to form pile or loop surface. Extra set of yarns forming the pile
may be cut to produce an erect pile on the face of fabric – Cut Pile – velvet or left uncut
to form loops on one or both sides of fabric- Uncut pile – terry.- Warp pile fabric – velvet, plushes, terry, velour.
- Weft pile fabric – velveteen, corduroy
-
Triaxial Fabric
Triaxial fabrics have 3 set of yarns, 2 warp & 1 filling. The warp yarns are placed
diagonally to each other by special attachments, through which the filling yarn is
interlaced. It is an ancient weave used in basket weaving. Stability against stretching in
all direction even bias, strong resistance, resistance to shear forces & raveling. Lighter,
longer life & less material required than biaxial fabrics. Three major weaves – basic
triaxial weave, basic basket triaxial weave & biplane weave.Uses – aerospace, industrial fabrics, sailcloth, balloon, truck covers, uniforms &
outerwear. -
Terry Fabric
A warp pile fabric in which loops are created, without positive assistance, by varying the relative positions of the fell and the reed. A high tension is applied to the ground warp and a very low tension to the pile warp.
-
Narrow Fabric
This is the type of any textile fabric made by interlacing fibers or yarns which does not exceed 45 cm ( in the U. K.) and does not exceed 30 cm ( in the U. S. A. and other countries). Narrow fabrics are characterized by the edges, which are the essential feature.
i see bi axial and triaxial, but it seems for the most strength, more axes would be required for the least stretch in more directions, ripstop, and possible gas, liquid impermeability… since a high strength comes from a circle, a hexaaxial or octaaxial weave would be better. and even better multi layer. could water filters be woven? or even gas filters with microfiber weaving. lets just hydrogen through by a molecular weave.
Wow, incredible weblog layout! How long have you ever been blogging for? you make blogging glance easy. The whole glance of your website is great, as neatly as the content!
How many shafts do renown fabric designers use?