English/Metric Conversion Table: Length
Inch | Yard | Centimeter | Meter | |
---|---|---|---|---|
Inch | 0.278 | 2.54 | 0.0254 | |
Yard | 36 | 91.44 | 0.9144 | |
Centimeter | 0.3937 | 0.011 | 0.01 | |
Meter | 39.37 | 1.094 | 100 |
English/Metric Conversion Table: Mass/Force
Ounce | Pound | Gram | Centi-Newton | Newton | |
---|---|---|---|---|---|
Ounce | 0.06237 | 28.3495 | 27.783 | 0.27802 | |
Pound | 15.96772 | 453.6 | 444.528 | 4.44528 | |
Gram | 0.0353 | 0.0022 | 0.98 | 0.0098 | |
Centi-Newton | 0.035904 | 0.002248 | 1.02 | 0.01 | |
Newton | 3.5904 | 0.2248 | 102 | 100 |
English/Metric Conversion Table: Saturated Steam Gauge Pressures
Pascal | Kilo-Pascal | Pounds per square inch | |
---|---|---|---|
Pascal(Pa) | 0.001 | 1.45 | |
Kilo-Pascal(kPa) | 1000 | 0.145 | |
Pounds per square inch(Psi) | 6895 | 6.895 |
English/Metric Conversion Table: Tenacity
gf/den | gf/tex | cN/tex | Rkm | |
---|---|---|---|---|
gf/den | 9.015 | 8.838 | 9.015 | |
gf/tex | 0.111 | 0.9807 | 1 | |
cN/tex | 0.113 | 1.02 | 1.02 | |
Rkm | 0.111 | 1 | 0.9807 |
Count Conversion Table
tex | dtex | den | Nm | NeC | NeL | |
---|---|---|---|---|---|---|
tex | dtex/10 | den/9 | 1000/Nm | 590.54/NeC | 1653.5/NeL | |
dtex | tex*10 | den/0.9 | 10000/Nm | 5905.4/NeC | 16535/NeL | |
den | tex*9 | dtex*0.9 | 9000/Nm | 5314.9/NeC | 14882/NeL | |
Nm | 1000/tex | 10000/dtex | 9000/den | NeC*1.6934 | NeL*0.6048 | |
NeC | 590.54/tex | 5905.4/dtex | 5314.9/den | Nm*0.5905 | NeL/2.8 | |
NeL | 1653.5/tex | 16535/dtex | 14882/den | Nm*1.6535 | NeC*2.8 |
Special Conversions
- TF = 95.67315 TM
- TM = 0.010452 TF
- Turns per inch t.p.i = 0.0254 * t.p.m
- Turns per meter t.p.m = 39.37 * t.p.i
- Fahrenheit °F = 1.8 * °C + 32
- Centigrade °C = 0.5556 * (°F – 32)
- Tkt Nm = 3000/Tkt tex
- Tkt tex = 3000/Tkt Nm
- m/kg = 2.016*yd/lb
- yd/lb = 0.496*m/kg
- yd2 = 0.836 m2
- m2 = 1.196 yd2
- oz/yd2 = 33.9* g/m2
- g/m2 = 0.0295* oz/yd2
- th/cm = 0.3937* th/in
- th/in = 2.54* th/cm
How we calculate of any yarn RKM from CSP ?
FOR MELANGE YARN 10/1 TO 40/1 CONTACT
OPEN END YARN AND RING SPUN YARN.
WHATSAPP/CALL: +92-300-2035287
FAWAD.AHMAD@MASOODTEXTILE.COM
how to covert Cn/dT to g/denier
Hello. I need to know, I am calculating RKM of yarn by multiplication of CLSP with 0.00645, then how I can convert RKM into Breaking Tenacity (cN/Tex)
you will get some reply
How to convert Newtown/Tex to gram/tex
How convert can /Tex in to csp
Please also tell me the formula which help us to calculate the CLSP yarn should be used for such strength
i need a little help
i need following strength specific fabrics
16/s x 12/s / 96 x 48, 3/1, cotton, 63″width
Tensile breaking strength (Strip Method)
Warp: 265 kg or 2599.65 Newton
Weft : 160 kg or 1569.60 Newton
What CLSP or strength of yarn should be to make such a strong fabrics. Please reply me on my email: mianghulamhaider@gmail.com