POST SPINNING
Afterthecompletespinningprocess, cones are being again twisted in post spinning section. In this, two cones are being used to wind up one cone with a higher twist. The method of twisting two or more single yarns is called doubling or folding or ply twisting. Such yarns are designated as doubled yarn, folded yarn, or plied yarn and the machines intended for the purpose are called doublers, ply-twisters of two-for-one (TFO) twisters.
TFO machines give a reverse or opposite twist that is being given in the spinning process i.e. Z- the twist is being given in the spinning department but after it is being rewarded in the TFO section, the cones are given S-twist.
The twist in the yarn is the number arrived by the ratio of the spindle speed to the delivery of the yarn. Both the factors are controlled by mechanical means and depend on the speed transmitted by the rotating parts.
S.No. | Technical Specification | |
1 | Machine used | Leewha, Prerna, Italy |
2 | Total no. of machines installed | 43 |
3 | Total no. of spindles in one machine | 144 spindles |
4 | Production | 42kg /shift |
5 | Total number of workers | 16/shift |
6 | The capacity of yarn twist | 8 ton per day |
7 | Speed | 7000rpm |
STEAMER
After cones are reminded in TFO machines, they are put into the steamer. It is done so as to avoid the snarling effect and also a twist of the yarn which is given is being set. The steamer also gives a conditioning effect to the yarn.
S.No. | Technical Specifications | |
1 | Capacity of steamer | 450kg-550kg |
2 | Time taken | 2 hours |
3 | The temperature required for wool and polyester | 90-95 ℃ |