Washing Techniques for Denim Jeans

Washing can be considered the final process in denim production and is the core of denim finishing. The washing of denim is directly related to the aesthetic, quality, and value of denim garments. In processing, sizing and coloration form the base of color in denim garments (Wang, 1995).

Blue Denim Fabrics

Word “denim” comes from fabric “serge de Nimes” made in France city of Nimes from where it originates. It has been used in America since the late 18th century, colored blue with indigo dye to make blue “jeans”, a type of cotton pants.