Knitting Quality Development
Set the loop for the finished fabric. The greige weight is a consequence, not a target.
— mm
Solved at the finished stitch density
The shrinkage figures are properties of a quality on a finishing route, not of a fabric type, and must be established from measured greige and finished samples rather than assumed - they drift with relaxation time, compactor setting and moisture. Weight gain in finishing is not independent of them: it is the reciprocal of the area factor, so if a measured gain contradicts the measured shrinkages, one measurement is wrong. This is a single jersey relation as written; on rib and interlock the stitch density must count loops on both beds or the calculated loop length will be out by a structure-dependent factor of around two. The finished density should come from a conditioned, fully relaxed laboratory sample - a density taken from fabric still under roll tension will produce a loop length that misses the target weight in the light direction. Residual shrinkage after laundering is a separate specification and is not addressed here.
Loop Length for a Target Finished Weight, Through Finishing Shrinkage — free, with the formula and a worked example, at Textile School.