Objectives of blow room
- To open the compressed bales of fibers
- Remove dirt and dust, broken leaf, seed particles or any other foreign impurities from the fibers
- To transfer the opened and cleaned fibers into a sheet form of definite width uniform weight per unit length which is called lap.
- To roll the lap of predetermined length into a cylindrical shape around a lap pin.
- To transfer the lap from the lap pin to a lap rod to a suitable and feed it to the subsequent m/c (carding).
The action of blow room line
- The action of opposing spikes
- The action of air currents
- Action of beaters
- Regulating action
Wastage in blow room
- Dropping
- Dust
- Filter waste
Faults in blow room
- Irregular lap
- Knocking off before completion of full lap
- Rough appearance of a full lap
- Lap sheet thicker at one side than the other
- Soft lap
- Lap licking
- Dropping under beater & grid bars
- Formation of conical lap
- Formation of split lap
- Barrel-shaped lap
- Ragged lap selvedges
Types of the beater in blow room
- Porcupine beater
- Bladed beater
- Krishner beater
Blow-room Video