Working of Nozzle of Airflow Dyeing Machine
The nozzle of an airflow dyeing machine (Figure 3) consists of an injector, annular mixing room, air pipe, nozzle body, and shell, etc. Dyeing liquor is atomized and jetted into the annular mixing room by the injector. At the same time, high-pressure air is pumped into an annular mixing room and mixed with the atomized dyeing liquor. After mixture, they are jetted at the fabric. During this process, the fabric is pulled to move forward by high-pressure air when it is dyed. Comparing with overflow dyeing machine, airflow dyeing machine does have a lower liquor ratio and better levelness.
Process and Technology Involved in Air-Dyeing
These are the most modern rope dyeing machines currently available on the market. The operating principle is similar to the jet dyeing system, but the fabric, guided by a motorized reel, is exposed inside the nozzle to a stream of forced air, blowing from one or two turbines (or fans) which take the air from inside. During the transport stage, or at the exit of the transport section, or, if necessary in both areas, the rope is sprayed with a controlled quantity of dyeing liquor; the atomized quantity of liquor slightly exceeds the one that the fiber can actually absorb. When the fabric folds in the perforated collection vat, it releases the excess liquor, which is recirculated by the special pump (Figure 4).
The fabric transport speed can be also very high (between 250 and 1000 m/min) while the liquor ratio could be, in theory, 1:1 to 1:2; in standard processing conditions the liquor ratio is 1:3-1:8. This machine usually allows a high temperature process.
The high speed of the fabric fed, together with the reduced liquor ratio, guarantee optimum dyeing results in very short times; it also reduces water consumption and the quantities of auxiliaries and dyes necessary for an optimum dyeing process, thus leading to considerable cost reduction (also with regard to wastewater treatment costs). This applies particularly to dying, above all in the case of dyes with low affinity for fibers and low exhaustion percentages.
However, sometimes the low liquor ratio could cause problems due to the poor solubility of some dyes and/or during subsequent post-dyeing washing process when higher liquor ratios would be more helpful.
These machines have also been designed for dyeing fabrics made of natural fibers, synthetic fibers, blends of man-made and elastic fibers, and micro-fiber fabrics; in reality, these machines have proved to be extremely suitable for dyeing man-made filament fabrics. While air feeding facilitates the continuous motion of the fabric and reduces possible defects due to rope folding, the fabric tends to pack on the bottom of the machine for the extremely reduced quantity of liquor, thus leading to permanent wrinkles.
This problem becomes clear above all for fabrics made of synthetic fibers, particularly when they have not been efficiently heat-set, and sometimes it is amplified by the water blade beating the fabric at the exit of the nozzle. These systems can process lots from 100 to 600-800 kgs, depending on the size of the machine and of the ropes.
Advantages of Airflow Dyeing Technology
Several advantages can be claimed by Air-flow dyeing over other conventional dyeing technologies. Air-Dyeing technology manages the application of color to textiles without the use of water. It is today’s sustainable alternative to traditional dyeing and decorating processes. Airflow is the key element of the technology, as air is an ideal transport medium.
The replacement of dye liquor with air as a method of transporting piece goods in jet-dyeing machines is a big step toward reducing water and chemicals consumption. Compared to the jet system in which the nozzles are filled with liquor, nozzle pressure is negligible, thus offering optimum protection of sensitive textile surfaces. At the same time, the use of the mass flow principle provides a major improvement in fabric hank laying, thus preventing creasing.
The moisture-saturated airflow ensures the uniform distribution of temperature on the fabric and in the machine, constituting a prerequisite for even and reproducible dyeing. Moreover, the low level of liquor in the dyeing boiler means the fabric is lighter than in conventional machinery and can, therefore, be accelerated quickly to high speeds. Thus, the risk of draft or strain is minimal, which is particularly advantageous with regard to the finishing of items containing elastane fibers.
The high transportation speeds of the fabric result in very short fabric turn time. High heating-up gradients are possible because a very low liquor ratio is maintained. The unique ability to use a hot drain system and rinsing with fresh water in a running wash system considerably reduces the time required for the dyeing process.
Some Specific Benefits are
- It does not pollute water in the color application process. By using air instead of water to convey dye, no hazardous waste is emitted and no water is wasted.
- It greatly reduces energy requirements, thereby lowering costs and satisfying the strictest standards of global responsibility.
- It does not use boilers, screen printing machines, drying ovens, or cleaning and scouring chemicals, thereby eliminating major sources of pollution.
- It eliminates water in the color application step and simplifies the process, creating revolutionary possibilities of new industry and employment in un-farmable, arid regions of the world.
- It gives consumers a way to choose style and sustainability at a realistic price at the point of purchase, thereby initiating world change.
- Air-Dye technology eliminates hazardous wastewater as a byproduct of dyeing fabric. Water scarcity affects one in three people on every continent and is getting worse as water needs rise with population growth, urbanization and increased usage by households and industries.
- Depending on the fabric, and type of dyeing, Air-Dye uses up to 95% less water, and up to 86% less energy, contributing 84% less to global warming, according to an independent assessment. Additionally, some companies state that with Air-Dye technology they can print to order which eliminates production excess and waste.
- Overall dyeing is cost reduced to a greater extent compared to traditional methods.
- Since Air-Dye process injects the dyes into the fabric and not on the fabric, bleaching and cleaning agents do not affect them. Using Air-Dyeing technology, for every 25,000 T-shirts sold, a company can save energy of 1,132,500 megajoules, water to the extent of 157,500 gallons, greenhouse emissions of 57, 500 (Kg CO2 equiv. emissions).
- The Airflow Dyeing is being especially suitable for the wet finishing of delicate cellulose and man-made-fiber knitwear and woven fabrics with a high percentage of elastane. Such fabrics are used in the automotive, lingerie, sports-leisure and swimwear segments.