Qiviut Fiber Musk-Ox/Musk-Oxen wool

Qiviut, pronounced kiv-ee-ute, is one of the finest natural fibers obtainable. Qiviut is the downy-soft underside wool from the arctic musk ox - oomingmak - umimmak in Greenlandic. Eight times warmer than wool and extraordinarily…