Home » Calculators » Wet Processing » Wet Processing (Dyeing & Printing) » Continuous Dyeing Range Dosing Pump Rate Calculator
Jump to a calculator 671 tools

Wet Processing

Continuous Dyeing Range Dosing Pump Rate Calculator

Put this calculator on your own site

Paste this where you want the calculator to appear. It works on any site — WordPress, Squarespace, Webflow, Ghost or plain HTML — and needs no JavaScript of yours. It carries a link back here, which is the only thing we ask for it.

See what it looks like

On a continuous range the pump must track the line. A fixed dose plus a speed change is a shade change.

Line Running conditions
m/min
m
g/m²
Application Padder and bath
%
g/L

Liquor Demand

— L/h

Volume the padder removes from the trough

Line & Pump

Fabric Throughput
— kg/h
Area Throughput
— m2/h
Chemical Consumption
— kg/h
Dosing Pump Setting
— mL/min

Trough volume should be as small as the machine allows. A large trough means the first metres after a stop carry a different concentration than the rest.

Using this calculator

About the Continuous Dyeing Range Dosing Pump Rate Calculator

The formula

This is the expression the tool evaluates. Every term is named underneath, with the unit it must be supplied in.

Liquor Demand
liquorRate = f( fabricSpeed, width, gsm, pickup, chemicalConc )

Each input feeds the expression evaluated in the browser; the symbol table below names every term and its unit.

Symbols used above
SymbolStands forUnit
fabricSpeedLine Speedm/min
widthFabric Widthm
gsmFabric Weightg/m²
pickupWet Pick-up%
chemicalConcChemical Concentrationg/L
liquorRateLiquor DemandL/h
fabricRateFabric Throughputkg/h
areaRateArea Throughputm2/h
chemicalRateChemical Consumptionkg/h
pumpRateDosing Pump SettingmL/min

How the result is derived

Step by step, from the values you type to the figure on screen.

  1. The 5 inputs are read from the form on every keystroke: Line Speed, Fabric Width, Fabric Weight, Wet Pick-up and Chemical Concentration.
  2. Each value is checked against the accepted range in the input table below. A value outside its range stops the calculation rather than producing a misleading figure — the results blank out and a message appears.
  3. The validated values are substituted into the expression above, which resolves Liquor Demand together with every supporting figure in one pass — no value is carried over from a previous entry.
  4. The supporting outputs — Fabric Throughput, Area Throughput, Chemical Consumption and Dosing Pump Setting — come from the same pass, so they always describe the same case as the headline figure.
  5. Results are rounded for display only. The full-precision value is used throughout the chain, so reading a rounded intermediate figure back into the tool by hand can shift the last digit.

What each input means

Where to read each value on the floor, the unit it must be in, and the range the tool accepts.

InputUnitAccepted rangeDefaultWhat it means
Line Speedm/min1 to 200 m/min40
Fabric Widthm0.1 to 5 m1.8
Fabric Weightg/m²10 to 1000 g/m²150
Wet Pick-up%10 to 200 %65
Chemical Concentrationg/L0.1 to 500 g/L50

What the tool returns

The headline figure and every supporting value it is built from.

OutputUnitWhat it tells you
Liquor Demand (headline result)L/hVolume the padder removes from the trough
Fabric Throughputkg/h
Area Throughputm2/h
Chemical Consumptionkg/h
Dosing Pump SettingmL/min

Worked example

Given

Line Speed
40 m/min
Fabric Width
1.8 m
Fabric Weight
150 g/m²
Wet Pick-up
65 %
Chemical Concentration
50 g/L

The tool loads with this case already solved — the Liquor Demand shown above is its answer. Change one value and the difference from this baseline is the sensitivity of the result to that variable.

How to use it

  1. Work through the input groups in order — Line and Application. The defaults are a realistic case, so you can change one value at a time and watch what moves.
  2. There is no calculate button. Every figure recalculates as you type or drag, which is what makes this usable for a what-if sweep rather than a single answer.
  3. Read Liquor Demand in the dark results panel — that is the headline figure, expressed in L/h.
  4. Check the supporting rows underneath (Fabric Throughput, Area Throughput, Chemical Consumption and Dosing Pump Setting) before acting on the headline — they are where an implausible input usually shows itself first.
  5. Reset to defaults returns every field to the reference case, which is the quickest way to check whether a surprising result came from the tool or from an input you had changed earlier.

Where this is used

  • Process planning — establishing Liquor Demand before a trial is booked, so machine time and material in Wet Processing (Dyeing & Printing) are committed against a calculated figure rather than an estimate.
  • Costing and quotation — Liquor Demand is an input to the cost sheet, and quoting from a worked number rather than a remembered one is what keeps a margin intact.
  • Troubleshooting — when the floor result drifts from plan, entering the measured values (starting with Line Speed) shows how much of the gap in Liquor Demand each variable explains.
  • Teaching and study — the accepted ranges bracket normal Wet Processing (Dyeing & Printing) practice, so moving one variable at a time shows the shape of the relationship rather than a single answer.

Assumptions and limits

  • Trough volume should be as small as the machine allows. A large trough means the first metres after a stop carry a different concentration than the rest.
  • Every input is bounded to the range normal practice occupies (Line Speed 1 to 200 m/min, Fabric Width 0.1 to 5 m and Fabric Weight 10 to 1000 g/m², and so on for the rest). Those bounds are guard rails against typing errors, not a claim that the formula fails one unit outside them.
  • The calculation is deterministic: the same inputs always give the same result. It carries no allowance for machine condition, operator skill, ambient conditions or lot-to-lot material variation unless an input above explicitly represents one.
  • Nothing is sent anywhere. The maths runs in your browser, so the numbers you type never leave the page.

Questions people ask

What do I need to know before using the Continuous Dyeing Range Dosing Pump Rate Calculator?

Have these to hand: Line Speed, Fabric Width, Fabric Weight, Wet Pick-up and Chemical Concentration. With those entered, the tool returns Liquor Demand immediately.

What exactly is Liquor Demand?

Volume the padder removes from the trough. It is reported in L/h. It is derived from Line Speed, Fabric Width, Fabric Weight, Wet Pick-up and Chemical Concentration, and is the figure the rest of the Wet Processing (Dyeing & Printing) calculation is built around.

Which units does this calculator expect?

Enter Line Speed in m/min, Fabric Width in m, Fabric Weight in g/m², Wet Pick-up in % and Chemical Concentration in g/L. Mixing unit systems is the most common cause of a result that looks an order of magnitude wrong — convert before typing, not after reading.

What are the other figures under the main result?

They are the intermediate quantities the calculation passes through: Fabric Throughput, Area Throughput, Chemical Consumption and Dosing Pump Setting. They are shown because a headline number nobody can trace is a number nobody trusts — checking them against your own expectation is the fastest way to confirm the inputs were read as you intended.

Can I rely on this for a production decision?

Trough volume should be as small as the machine allows. A large trough means the first metres after a stop carry a different concentration than the rest. Treat the output as an engineering estimate that narrows the trial window, not as a substitute for the trial.

Scroll to Top

Follow on WhatsApp

Scan with your phone’s camera to open the channel, then tap Follow.

QR code for the WhatsApp channelOr open WhatsApp on this device