Jump to a calculator 671 tools
Continuous Dyeing
Pad-Thermosol Sublimation Loss Calculator
Every degree above the fixation window buys speed and pays for it in dye going up the stack. The loss doubles long before the shade does.
Sublimation Loss
— %
Share of applied dye lost during the cure
Loss Balance
- Temperature-Corrected Loss Rate
- — %/min
- Excess Over Reference
- — °C
- Dye Lost
- — % owf
- Dye Retained on Cloth
- — % owf
- Retention
- — %
The doubling interval and reference rate are dye-specific and must come from your own thermosol trials — a low-energy disperse dye and a high-energy one behave nothing alike. Sublimed dye is an emissions issue as well as a cost: check the exhaust duty.
Using this calculator
About the Pad-Thermosol Sublimation Loss Calculator
The formula
This is the expression the tool evaluates. Every term is named underneath, with the unit it must be supplied in.
sublimationLoss = f( curingTemp, curingTime, referenceTemp, referenceLossRate, doublingInterval, dyeApplied )Each input feeds the expression evaluated in the browser; the symbol table below names every term and its unit.
| Symbol | Stands for | Unit |
|---|---|---|
curingTemp | Curing Temperature | °C |
curingTime | Dwell Time | s |
referenceTemp | Reference Temperature | °C |
referenceLossRate | Loss Rate at Reference | %/min |
doublingInterval | Doubling Interval | °C |
dyeApplied | Dye Applied | % owf |
sublimationLoss | Sublimation Loss | % |
lossRate | Temperature-Corrected Loss Rate | %/min |
tempExcess | Excess Over Reference | °C |
dyeLost | Dye Lost | % owf |
dyeRetained | Dye Retained on Cloth | % owf |
retention | Retention | % |
How the result is derived
Step by step, from the values you type to the figure on screen.
- The 6 inputs are read from the form on every keystroke: Curing Temperature, Dwell Time, Reference Temperature, Loss Rate at Reference, Doubling Interval and Dye Applied.
- Each value is checked against the accepted range in the input table below. A value outside its range stops the calculation rather than producing a misleading figure — the results blank out and a message appears.
- The validated values are substituted into the expression above, which resolves Sublimation Loss together with every supporting figure in one pass — no value is carried over from a previous entry.
- The supporting outputs — Temperature-Corrected Loss Rate, Excess Over Reference, Dye Lost, Dye Retained on Cloth and Retention — come from the same pass, so they always describe the same case as the headline figure.
- Results are rounded for display only. The full-precision value is used throughout the chain, so reading a rounded intermediate figure back into the tool by hand can shift the last digit.
What each input means
Where to read each value on the floor, the unit it must be in, and the range the tool accepts.
| Input | Unit | Accepted range | Default | What it means |
|---|---|---|---|---|
| Curing Temperature | °C | 100 to 260 °C | 205 | |
| Dwell Time | s | 5 to 600 s | 60 | |
| Reference Temperature | °C | 100 to 260 °C | 190 | |
| Loss Rate at Reference | %/min | 0.01 to 50 %/min | 0.8 | |
| Doubling Interval | °C | 1 to 60 °C | 15 | Temperature rise that doubles the sublimation rate. |
| Dye Applied | % owf | 0.01 to 20 % owf | 2.5 |
What the tool returns
The headline figure and every supporting value it is built from.
| Output | Unit | What it tells you |
|---|---|---|
| Sublimation Loss (headline result) | % | Share of applied dye lost during the cure |
| Temperature-Corrected Loss Rate | %/min | |
| Excess Over Reference | °C | |
| Dye Lost | % owf | |
| Dye Retained on Cloth | % owf | |
| Retention | % |
Worked example
Given
- Curing Temperature
- 205 °C
- Dwell Time
- 60 s
- Reference Temperature
- 190 °C
- Loss Rate at Reference
- 0.8 %/min
- Doubling Interval
- 15 °C
- Dye Applied
- 2.5 % owf
The tool loads with this case already solved — the Sublimation Loss shown above is its answer. Change one value and the difference from this baseline is the sensitivity of the result to that variable.
How to use it
- Work through the input groups in order — Curing, Calibration and Recipe. The defaults are a realistic case, so you can change one value at a time and watch what moves.
- There is no calculate button. Every figure recalculates as you type or drag, which is what makes this usable for a what-if sweep rather than a single answer.
- Read Sublimation Loss in the dark results panel — that is the headline figure, expressed in %.
- Check the supporting rows underneath (Temperature-Corrected Loss Rate, Excess Over Reference, Dye Lost, Dye Retained on Cloth and Retention) before acting on the headline — they are where an implausible input usually shows itself first.
- Reset to defaults returns every field to the reference case, which is the quickest way to check whether a surprising result came from the tool or from an input you had changed earlier.
Where this is used
- Process planning — establishing Sublimation Loss before a trial is booked, so machine time and material in Advanced Colour Physics & Wet Processing are committed against a calculated figure rather than an estimate.
- Costing and quotation — Sublimation Loss is an input to the cost sheet, and quoting from a worked number rather than a remembered one is what keeps a margin intact.
- Troubleshooting — when the floor result drifts from plan, entering the measured values (starting with Curing Temperature) shows how much of the gap in Sublimation Loss each variable explains.
- Teaching and study — the accepted ranges bracket normal Advanced Colour Physics & Wet Processing practice, so moving one variable at a time shows the shape of the relationship rather than a single answer.
Assumptions and limits
- The doubling interval and reference rate are dye-specific and must come from your own thermosol trials — a low-energy disperse dye and a high-energy one behave nothing alike. Sublimed dye is an emissions issue as well as a cost: check the exhaust duty.
- Every input is bounded to the range normal practice occupies (Curing Temperature 100 to 260 °C, Dwell Time 5 to 600 s and Reference Temperature 100 to 260 °C, and so on for the rest). Those bounds are guard rails against typing errors, not a claim that the formula fails one unit outside them.
- The calculation is deterministic: the same inputs always give the same result. It carries no allowance for machine condition, operator skill, ambient conditions or lot-to-lot material variation unless an input above explicitly represents one.
- Nothing is sent anywhere. The maths runs in your browser, so the numbers you type never leave the page.
Questions people ask
What do I need to know before using the Pad-Thermosol Sublimation Loss Calculator?
Have these to hand: Curing Temperature, Dwell Time, Reference Temperature, Loss Rate at Reference, Doubling Interval and Dye Applied. With those entered, the tool returns Sublimation Loss immediately.
What exactly is Sublimation Loss?
Share of applied dye lost during the cure. It is reported in %. It is derived from Curing Temperature, Dwell Time, Reference Temperature, Loss Rate at Reference, Doubling Interval and Dye Applied, and is the figure the rest of the Advanced Colour Physics & Wet Processing calculation is built around.
Which units does this calculator expect?
Enter Curing Temperature in °C, Dwell Time in s, Reference Temperature in °C, Loss Rate at Reference in %/min, Doubling Interval in °C and Dye Applied in % owf. Mixing unit systems is the most common cause of a result that looks an order of magnitude wrong — convert before typing, not after reading.
What are the other figures under the main result?
They are the intermediate quantities the calculation passes through: Temperature-Corrected Loss Rate, Excess Over Reference, Dye Lost, Dye Retained on Cloth and Retention. They are shown because a headline number nobody can trace is a number nobody trusts — checking them against your own expectation is the fastest way to confirm the inputs were read as you intended.
Can I rely on this for a production decision?
The doubling interval and reference rate are dye-specific and must come from your own thermosol trials — a low-energy disperse dye and a high-energy one behave nothing alike. Sublimed dye is an emissions issue as well as a cost: check the exhaust duty. Treat the output as an engineering estimate that narrows the trial window, not as a substitute for the trial.