Specification
| Parameter | Value | As published |
|---|---|---|
| Number of electrospinning units | 1 | |
| Number of application modules | 2 | |
| Total number of spinning electrodes | 8 | 4 per module |
| Spinning electrode width | 1600 mm | adjustable width 1000-1600 mm |
| Electrospinning voltage | 0–140 kV | |
| Unwinding speed | 0,2–40,0 m/min. | |
| Distance of the spinning electrode to the substrate | 150–250 mm | |
| The distance of the wires of the collecting electrode above the substrate | 30–130 mm | |
| Electrical Consumption | 5 kW | |
| Height | 2930 mm | |
| Width | 3200 mm | |
| Length | 2600 mm | |
| Weight | 2500 kg | |
| Temperature | 20–30 °C | |
| Humidity | 20–40 % RH | |
| Startup time | 20 min. | |
| Time required to fill the polymer | 15 minutes | |
| Tank volume | 60 litres | 2×30 litres |
| Monthly maintenance allowance | 15 hours | |
| Serving staff | 1.5 person/shift | |
| Production premises requirements | 200 m² | 10×20 m |
| Minimum ceiling height | 4 m |
Read from the builder's published page: www.elmarco.com, on 2026-11-02.
Check against the machine before you buy or budget on it. Builders publish a range and a configuration; the machine on your floor may be a different variant, may have been rebuilt, and may not carry the options these figures assume. This register records what the builder published, not what any individual machine does.
Related machines
Also from Elmarco
Other machines of this kind: Spunbond and meltblown
Report incorrect information on this page
Tell us what is wrong and we will check it against the source. Reports are private, are never published, and go to an editor rather than into a comment thread.