Mesdan Hand-operated Twist Tester 2531D is a yarn testing instrument, still in its builder’s current range. Its builder lists pretension up to 70 cN and test length 1 to 50 cm. Yarn testing instruments measure yarn and fibre properties such as evenness, imperfections, hairiness, tensile strength, elongation, count and twist, as well as fibre length and fineness.
Yarn testingTesting and laboratoryIn the builder's current range
Key specifications
Specifications incomplete: 1 of 5 key figures recorded
- Yarn test speed (evenness / hairiness)—
- Force capacity—
- Tensile (crosshead) speed—
- Yarn count range—
- Test standardsASTM D1422, ASTM D1423, UNI 9067, UNI 9277, UNI 9069, UNI EN ISO 2061, ISO 7211-4, ISO 17202, ISO 2061
- Gauge length10–500 mm
- Class
- Yarn testing
- Process stage
- Testing and laboratory
- Lifecycle
- In the builder's current range
Specification
| Parameter | Value |
|---|---|
| Test length | 1 to 50 cm |
| Pretension | up to 70 cN |
| Accuracy | ±1 turn |
| Reference standards | ASTM D1422, ASTM D1423, UNI 9067, UNI 9277, UNI 9069, UNI EN ISO 2061, ISO 7211-4, ISO 17202, ISO 2061 |
Read from the builder's published page: mesdan.com, on 2026-11-16.
Check against the machine before you buy or budget on it. Builders publish a range and a configuration; the machine on your floor may be a different variant, may have been rebuilt, and may not carry the options these figures assume. This register records what the builder published, not what any individual machine does.
The record
- Read from
- mesdan.com,
- Checked by
- Textile School,
- Last changed
Related machines
Also from Mesdan
Other machines of this kind: Yarn testing
Report incorrect information on this page