Home » Machinery specifications » Mesdan Micronaire 199C

Mesdan Micronaire 199C

Checked by an editor

Mesdan Micronaire 199C is a fibre testing instrument, still in its builder’s current range. Its builder lists fineness range 2.5 to 7 micronaire index. Fibre testing instruments measure raw fibre before it is spun: length and length uniformity, fineness or micronaire, maturity, strength, trash, neps and colour grade.

Fibre testingTesting and laboratoryIn the builder's current range

Specification

ParameterValue
Fineness range2.5 to 7 micronaire index
Sample weightabout 2.5 grams
Reference standardsISO 2403, ASTM D1448, BS 3181-1

Read from the builder's published page: mesdan.com, on 2026-11-16.

Check against the machine before you buy or budget on it. Builders publish a range and a configuration; the machine on your floor may be a different variant, may have been rebuilt, and may not carry the options these figures assume. This register records what the builder published, not what any individual machine does.

The record

Read from
mesdan.com,
Checked by
Textile School,
Last changed

All machinery specifications

Related machines

Report incorrect information on this page

Tell us what is wrong and we will check it against the source. Reports are private, are never published, and go to an editor rather than into a comment thread.

Scroll to Top

Follow on WhatsApp

Scan with your phone’s camera to open the channel, then tap Follow.

QR code for the WhatsApp channelOr open WhatsApp on this device