Home » Machinery specifications » Unuo Instruments UI-FT19

Unuo Instruments UI-FT19

Manufacturer supplied

Unuo Instruments UI-FT19 is a piece of laboratory equipment used in textile testing and quality control, still in its builder’s current range. Its builder lists speed 47.5 ± 5 r/min, diameter of abrading base 125±5mm and test positions 4, 6, 8, 9. Laboratory equipment covers the instruments and small-scale machines a mill or research laboratory uses away from the production line: colour measurement, sample conditioning and preparation, chemical checks, and laboratory or pilot units for developing a process before it is scaled up.

Specifications supplied by Unuo Instruments Co., Ltd on 2026-11-06, from a confirmed address at their own domain. The figures are theirs and have not been independently checked against a source.

Laboratory equipmentTesting and laboratoryIn the builder's current range

Key specifications

Specifications incomplete: 0 of 5 key figures recorded

  • Samples / beakers per run—
  • Max. temperature—
  • Measuring range—
  • Accuracy—
  • Test standards—
  • Installed power1 kW

Specification

ParameterValue
Sample sizeDiameter 38mm
Test Positions4, 6, 8, 9
Size of abrasion head28.66 ± 0.25mm (Exposed area of specimen holder: 645±5mm2)
Pressure595 ± 5g (9kPa) ; 795 ± 7g (12kPa)
Speed47.5 ± 5 r/min
Press Weight2.5±0.5kg;diameter:120±1mm
Size of Lissajous figure60±1mm, 24mm
Diameter of abrading base125±5mm
Power1∮ 220V

Read from the builder's published page: www.unuo-instruments.com, on 2026-11-07.

Check against the machine before you buy or budget on it. Builders publish a range and a configuration; the machine on your floor may be a different variant, may have been rebuilt, and may not carry the options these figures assume. This register records what the builder published, not what any individual machine does.

The record

Read from
www.unuo-instruments.com,
Checked by
Textile School,
Supplied by
Unuo Instruments Co., Ltd,
Last changed

All machinery specifications

Related machines

Also from Unuo Instruments

Report incorrect information on this page

Tell us what is wrong and we will check it against the source. Reports are private, are never published, and go to an editor rather than into a comment thread.

Scroll to Top

Follow on WhatsApp

Scan with your phone’s camera to open the channel, then tap Follow.

QR code for the WhatsApp channelOr open WhatsApp on this device