Jump to a calculator 671 tools
Yarn Spinning & Preparation
Universal Yarn Count Converter
Pick the system you are quoting in. Every other system updates instantly.
Linear Density
— tex
Grams per 1000 metres — the SI reference
Equivalent Counts
- English Cotton
- — Ne
- Metric
- — Nm
- Denier
- — den
- Decitex
- — dtex
- Worsted
- — NeK
- Jute
- — lb/spy
Indirect systems (Ne, Nm, worsted) rise as the yarn gets finer; direct systems (tex, denier, jute) rise as it gets coarser. Always state the system when quoting a count.
Using this calculator
About the Universal Yarn Count Converter
The formula
This is the expression the tool evaluates. Every term is named underneath, with the unit it must be supplied in.
tex = 590.5 / Ne = 1000 / Nm = 885.8 / worsted = dtex / 10 = denier / 9 = jute / 0.029029Converting between seven systems pairwise would need 21 formulas. Converting each into tex and back out needs seven, and there is only one place a constant can be wrong.
Ne = 590.5 / tex Nm = 1000 / tex worsted = 885.8 / texThese count how many fixed-length hanks make up a unit of mass, so they rise as the yarn gets finer.
denier = tex x 9 dtex = tex x 10 jute = tex x 0.029029These measure the mass of a fixed length, so they rise as the yarn gets coarser. The jute factor is the mass in pounds of a 14,400 yard spyndle.
| Symbol | Stands for | Unit |
|---|---|---|
system | Counting System | — |
value | Count Value | — |
tex | Linear Density | tex |
ne | English Cotton | Ne |
nm | Metric | Nm |
denier | Denier | den |
dtex | Decitex | dtex |
worsted | Worsted | NeK |
jute | Jute | lb/spy |
How the result is derived
Step by step, from the values you type to the figure on screen.
- The chosen system and value are converted into tex, which is grams per 1000 metres and the SI reference for linear density.
- A non-positive or non-finite tex stops the conversion rather than propagating nonsense into six other systems.
- Every other system is then generated from that single tex value, so all seven outputs are guaranteed to describe the same yarn.
- The constants are fixed definitions, not measurements: 590.5 comes from 840 yard hanks per pound, 885.8 from 560 yard worsted hanks per pound, and 9 from 9000 metres per gram of denier.
What each input means
Where to read each value on the floor, the unit it must be in, and the range the tool accepts.
| Input | Unit | Accepted range | Default | What it means |
|---|---|---|---|---|
| Counting System | — | Ne — English cotton (indirect) · Nm — Metric (indirect) · Tex — g per 1000 m (direct) · Dtex — g per 10000 m (direct) · Denier — g per 9000 m (direct) · Worsted — 560 yd hanks per lb · Jute — lb per 14400 yd spyndle | 1 | |
| Count Value | — | 0.0001 to 100000 | 40 |
What the tool returns
The headline figure and every supporting value it is built from.
| Output | Unit | What it tells you |
|---|---|---|
| Linear Density (headline result) | tex | Grams per 1000 metres — the SI reference |
| English Cotton | Ne | |
| Metric | Nm | |
| Denier | den | |
| Decitex | dtex | |
| Worsted | NeK | |
| Jute | lb/spy |
Worked example
Given
- System
- Ne — English cotton
- Value
- 40
Substituting
tex = 590.5 / 40 = 14.7625Nm = 1000 / 14.7625 = 67.74denier = 14.7625 x 9 = 132.86worsted = 885.8 / 14.7625 = 60.00Answer
- Tex
- 14.76
- Nm
- 67.74
- Denier
- 132.86
- Dtex
- 147.63
- Worsted
- 60.00
- Jute
- 0.43
A 40s cotton yarn is a 60s worsted, a 133 denier and a 14.76 tex. All four describe the identical yarn — only the reference length and the direction of the scale change.
How to use it
- Work through the input groups in order — Known Count. The defaults are a realistic case, so you can change one value at a time and watch what moves.
- There is no calculate button. Every figure recalculates as you type or drag, which is what makes this usable for a what-if sweep rather than a single answer.
- Read Linear Density in the dark results panel — that is the headline figure, expressed in tex.
- Check the supporting rows underneath (English Cotton, Metric, Denier, Decitex, Worsted and Jute) before acting on the headline — they are where an implausible input usually shows itself first.
- Reset to defaults returns every field to the reference case, which is the quickest way to check whether a surprising result came from the tool or from an input you had changed earlier.
Where this is used
- Reading a supplier quotation written in a system your mill does not use, without a conversion error becoming a purchase error.
- Filament and staple in one specification — filament is quoted in denier or dtex, staple yarn in Ne or Nm, and blends have to be reconciled.
- Technical and regional specifications: worsted for wool, jute for packaging and geotextiles, tex wherever an ISO test method is being quoted.
- Cost comparison — yarn price per kilogram is only comparable once counts are on a common basis.
Reading the result
Typical bands and what each one is telling you.
| Value | What it indicates |
|---|---|
| Under 10 tex | Very fine — high count shirting, fine filament, sewing thread components. |
| 10 to 25 tex | The apparel mainstream: 24s to 60s Ne. |
| 25 to 60 tex | Bottomweight, denim, heavy knits, coarse count yarn. |
| Above 60 tex | Industrial: carpet, technical textiles, cordage components, jute. |
Assumptions and limits
- Indirect systems (Ne, Nm, worsted) rise as the yarn gets finer; direct systems (tex, denier, jute) rise as it gets coarser. Always state the system when quoting a count.
- Every input is bounded to the range normal practice occupies (Counting System Ne — English cotton (indirect) · Nm — Metric (indirect) · Tex — g per 1000 m (direct) · Dtex — g per 10000 m (direct) · Denier — g per 9000 m (direct) · Worsted — 560 yd hanks per lb · Jute — lb per 14400 yd spyndle and Count Value 0.0001 to 100000, and so on for the rest). Those bounds are guard rails against typing errors, not a claim that the formula fails one unit outside them.
- The calculation is deterministic: the same inputs always give the same result. It carries no allowance for machine condition, operator skill, ambient conditions or lot-to-lot material variation unless an input above explicitly represents one.
- Nothing is sent anywhere. The maths runs in your browser, so the numbers you type never leave the page.
Standards and further reading
- ISO 1144 — the tex system for linear density, the reference every other system is defined against here.
- ISO 2060 / ASTM D1907 — determination of yarn linear density by the skein method.
- ASTM D2260 — conversion tables for yarn number, the printed ancestor of this calculator.
On this site
Articles that explain what this tool calculates.
Questions people ask
What is the difference between a direct and an indirect system?
A direct system fixes the length and measures mass — tex, dtex, denier and jute. A larger number means a coarser yarn. An indirect system fixes the mass and measures length — Ne, Nm and worsted. A larger number means a finer yarn. Half of all count confusion is this one distinction.
Where does the constant 590.5 come from?
From the definition of the English cotton count: the number of 840 yard hanks in one pound. Convert 840 yards to metres and one pound to grams and the ratio comes out at 590.5 grams per 1000 metres for a 1s yarn.
Should I quote denier or dtex?
Dtex, in any new specification — it is the decitex member of the tex family, which is the ISO system. Denier survives in trade and in legacy specifications; the numbers differ by a factor of 1.111, which is small enough to slip past a careless reading.