Home » Calculators » Knitting » Advanced Knitting & Hosiery » Fleece & Terry Knit Loop Length and Plating Optimizer
Jump to a calculator 671 tools

Circular Knitting

Fleece & Terry Knit Loop Length and Plating Optimizer

Put this calculator on your own site

Paste this where you want the calculator to appear. It works on any site — WordPress, Squarespace, Webflow, Ghost or plain HTML — and needs no JavaScript of yours. It carries a link back here, which is the only thing we ask for it.

See what it looks like

The pile yarn is usually two thirds of the weight and nearly all of the hand. The face and tie yarns are what stop it pulling out.

Loop Lengths Per needle
mm
mm
mm
Yarn Counts Per stream
tex
tex
tex
Fabric Stitch density
courses/cm
wales/cm

Fabric Areal Weight

— g/m²

All three yarn streams, before brushing

Stream Balance

Face Yarn Weight
— g/m²
Tie Yarn Weight
— g/m²
Pile Yarn Weight
— g/m²
Pile Height
— mm
Pile Proportion of Weight
— %

Weight before brushing and finishing. Brushing breaks pile loops and sheds fibre, so the finished fabric weighs less than this while feeling considerably thicker.

Using this calculator

About the Fleece & Terry Knit Loop Length and Plating Optimizer

The formula

This is the expression the tool evaluates. Every term is named underneath, with the unit it must be supplied in.

Fabric Areal Weight
totalGsm = f( faceLoopLength, tieLoopLength, pileLoopLength, faceTex, tieTex, pileTex, coursesPerCm, walesPerCm )

Each input feeds the expression evaluated in the browser; the symbol table below names every term and its unit.

Symbols used above
SymbolStands forUnit
faceLoopLengthFace Yarn Loop Lengthmm
tieLoopLengthTie Yarn Loop Lengthmm
pileLoopLengthPile Yarn Loop Lengthmm
faceTexFace Yarntex
tieTexTie Yarntex
pileTexPile Yarntex
coursesPerCmCourses per cmcourses/cm
walesPerCmWales per cmwales/cm
totalGsmFabric Areal Weightg/m²
faceGsmFace Yarn Weightg/m²
tieGsmTie Yarn Weightg/m²
pileGsmPile Yarn Weightg/m²
pileHeightPile Heightmm
pileProportionPile Proportion of Weight%

How the result is derived

Step by step, from the values you type to the figure on screen.

  1. The 8 inputs are read from the form on every keystroke: Face Yarn Loop Length, Tie Yarn Loop Length, Pile Yarn Loop Length, Face Yarn, Tie Yarn, Pile Yarn, Courses per cm and Wales per cm.
  2. Each value is checked against the accepted range in the input table below. A value outside its range stops the calculation rather than producing a misleading figure — the results blank out and a message appears.
  3. The validated values are substituted into the expression above, which resolves Fabric Areal Weight together with every supporting figure in one pass — no value is carried over from a previous entry.
  4. The supporting outputs — Face Yarn Weight, Tie Yarn Weight, Pile Yarn Weight, Pile Height and Pile Proportion of Weight — come from the same pass, so they always describe the same case as the headline figure.
  5. Results are rounded for display only. The full-precision value is used throughout the chain, so reading a rounded intermediate figure back into the tool by hand can shift the last digit.

What each input means

Where to read each value on the floor, the unit it must be in, and the range the tool accepts.

InputUnitAccepted rangeDefaultWhat it means
Face Yarn Loop Lengthmm0.5 to 30 mm2.8
Tie Yarn Loop Lengthmm0.5 to 30 mm2.2
Pile Yarn Loop Lengthmm0.5 to 60 mm6.5
Face Yarntex1 to 500 tex20
Tie Yarntex1 to 500 tex10
Pile Yarntex1 to 500 tex30
Courses per cmcourses/cm1 to 60 courses/cm14
Wales per cmwales/cm1 to 60 wales/cm10

What the tool returns

The headline figure and every supporting value it is built from.

OutputUnitWhat it tells you
Fabric Areal Weight (headline result)g/m²All three yarn streams, before brushing
Face Yarn Weightg/m²
Tie Yarn Weightg/m²
Pile Yarn Weightg/m²
Pile Heightmm
Pile Proportion of Weight%

Worked example

Given

Face Yarn Loop Length
2.8 mm
Tie Yarn Loop Length
2.2 mm
Pile Yarn Loop Length
6.5 mm
Face Yarn
20 tex
Tie Yarn
10 tex
Pile Yarn
30 tex
Courses per cm
14 courses/cm
Wales per cm
10 wales/cm

The tool loads with this case already solved — the Fabric Areal Weight shown above is its answer. Change one value and the difference from this baseline is the sensitivity of the result to that variable.

How to use it

  1. Work through the input groups in order — Loop Lengths, Yarn Counts and Fabric. The defaults are a realistic case, so you can change one value at a time and watch what moves.
  2. There is no calculate button. Every figure recalculates as you type or drag, which is what makes this usable for a what-if sweep rather than a single answer.
  3. Read Fabric Areal Weight in the dark results panel — that is the headline figure, expressed in g/m².
  4. Check the supporting rows underneath (Face Yarn Weight, Tie Yarn Weight, Pile Yarn Weight, Pile Height and Pile Proportion of Weight) before acting on the headline — they are where an implausible input usually shows itself first.
  5. Reset to defaults returns every field to the reference case, which is the quickest way to check whether a surprising result came from the tool or from an input you had changed earlier.

Where this is used

  • Process planning — establishing Fabric Areal Weight before a trial is booked, so machine time and material in Advanced Knitting & Hosiery are committed against a calculated figure rather than an estimate.
  • Costing and quotation — Fabric Areal Weight is an input to the cost sheet, and quoting from a worked number rather than a remembered one is what keeps a margin intact.
  • Troubleshooting — when the floor result drifts from plan, entering the measured values (starting with Face Yarn Loop Length) shows how much of the gap in Fabric Areal Weight each variable explains.
  • Teaching and study — the accepted ranges bracket normal Advanced Knitting & Hosiery practice, so moving one variable at a time shows the shape of the relationship rather than a single answer.

Assumptions and limits

  • Weight before brushing and finishing. Brushing breaks pile loops and sheds fibre, so the finished fabric weighs less than this while feeling considerably thicker.
  • Every input is bounded to the range normal practice occupies (Face Yarn Loop Length 0.5 to 30 mm, Tie Yarn Loop Length 0.5 to 30 mm and Pile Yarn Loop Length 0.5 to 60 mm, and so on for the rest). Those bounds are guard rails against typing errors, not a claim that the formula fails one unit outside them.
  • The calculation is deterministic: the same inputs always give the same result. It carries no allowance for machine condition, operator skill, ambient conditions or lot-to-lot material variation unless an input above explicitly represents one.
  • Nothing is sent anywhere. The maths runs in your browser, so the numbers you type never leave the page.

On this site

Articles that explain what this tool calculates.

Questions people ask

What do I need to know before using the Fleece & Terry Knit Loop Length and Plating Optimizer?

Have these to hand: Face Yarn Loop Length, Tie Yarn Loop Length, Pile Yarn Loop Length, Face Yarn, Tie Yarn, Pile Yarn, Courses per cm and Wales per cm. With those entered, the tool returns Fabric Areal Weight immediately.

What exactly is Fabric Areal Weight?

All three yarn streams, before brushing. It is reported in g/m². It is derived from Face Yarn Loop Length, Tie Yarn Loop Length, Pile Yarn Loop Length, Face Yarn, Tie Yarn, Pile Yarn, Courses per cm and Wales per cm, and is the figure the rest of the Advanced Knitting & Hosiery calculation is built around.

Which units does this calculator expect?

Enter Face Yarn Loop Length in mm, Tie Yarn Loop Length in mm, Pile Yarn Loop Length in mm, Face Yarn in tex, Tie Yarn in tex, Pile Yarn in tex, Courses per cm in courses/cm and Wales per cm in wales/cm. Mixing unit systems is the most common cause of a result that looks an order of magnitude wrong — convert before typing, not after reading.

What are the other figures under the main result?

They are the intermediate quantities the calculation passes through: Face Yarn Weight, Tie Yarn Weight, Pile Yarn Weight, Pile Height and Pile Proportion of Weight. They are shown because a headline number nobody can trace is a number nobody trusts — checking them against your own expectation is the fastest way to confirm the inputs were read as you intended.

Can I rely on this for a production decision?

Weight before brushing and finishing. Brushing breaks pile loops and sheds fibre, so the finished fabric weighs less than this while feeling considerably thicker. Treat the output as an engineering estimate that narrows the trial window, not as a substitute for the trial.

Scroll to Top

Follow on WhatsApp

Scan with your phone’s camera to open the channel, then tap Follow.