Jump to a calculator 671 tools
Testing & Quality Control
Tear to Tensile Strength Ratio Calculator
A tightly set fabric can pass tensile and fail tear badly. The ratio is where that shows.
Tear to Tensile Ratio
— %
Tear strength as a share of tensile strength
Normalised Strength
- Tear Index
- — mN·m²/g
- Tensile per Unit Weight
- — N per g/m²
- Tear per Unit Weight
- — N per g/m²
- Margin over Minimum
- — %
Tear strength depends on yarn mobility. Resin finishing and very high sett both lock yarns in place and cut tear strength sharply while tensile barely moves.
Using this calculator
About the Tear to Tensile Strength Ratio Calculator
The formula
This is the expression the tool evaluates. Every term is named underneath, with the unit it must be supplied in.
ratio = f( tensileStrength, tearStrength, gsm, minRatio )Each input feeds the expression evaluated in the browser; the symbol table below names every term and its unit.
| Symbol | Stands for | Unit |
|---|---|---|
tensileStrength | Tensile Breaking Strength | N |
tearStrength | Tear Strength | N |
gsm | Fabric Weight | g/m² |
minRatio | Minimum Tear/Tensile Ratio | % |
ratio | Tear to Tensile Ratio | % |
tearIndex | Tear Index | mN·m²/g |
tensilePerGsm | Tensile per Unit Weight | N per g/m² |
tearPerGsm | Tear per Unit Weight | N per g/m² |
marginOverMinimum | Margin over Minimum | % |
How the result is derived
Step by step, from the values you type to the figure on screen.
- The 4 inputs are read from the form on every keystroke: Tensile Breaking Strength, Tear Strength, Fabric Weight and Minimum Tear/Tensile Ratio.
- Each value is checked against the accepted range in the input table below. A value outside its range stops the calculation rather than producing a misleading figure — the results blank out and a message appears.
- The validated values are substituted into the expression above, which resolves Tear to Tensile Ratio together with every supporting figure in one pass — no value is carried over from a previous entry.
- The supporting outputs — Tear Index, Tensile per Unit Weight, Tear per Unit Weight and Margin over Minimum — come from the same pass, so they always describe the same case as the headline figure.
- Results are rounded for display only. The full-precision value is used throughout the chain, so reading a rounded intermediate figure back into the tool by hand can shift the last digit.
What each input means
Where to read each value on the floor, the unit it must be in, and the range the tool accepts.
| Input | Unit | Accepted range | Default | What it means |
|---|---|---|---|---|
| Tensile Breaking Strength | N | 1 to 10000 N | 450 | |
| Tear Strength | N | 0.1 to 1000 N | 22 | |
| Fabric Weight | g/m² | 10 to 1000 g/m² | 180 | |
| Minimum Tear/Tensile Ratio | % | 0.1 to 50 % | 4 |
What the tool returns
The headline figure and every supporting value it is built from.
| Output | Unit | What it tells you |
|---|---|---|
| Tear to Tensile Ratio (headline result) | % | Tear strength as a share of tensile strength |
| Tear Index | mN·m²/g | |
| Tensile per Unit Weight | N per g/m² | |
| Tear per Unit Weight | N per g/m² | |
| Margin over Minimum | % |
Worked example
Given
- Tensile Breaking Strength
- 450 N
- Tear Strength
- 22 N
- Fabric Weight
- 180 g/m²
- Minimum Tear/Tensile Ratio
- 4 %
The tool loads with this case already solved — the Tear to Tensile Ratio shown above is its answer. Change one value and the difference from this baseline is the sensitivity of the result to that variable.
How to use it
- Work through the input groups in order — Test Results and Specification. The defaults are a realistic case, so you can change one value at a time and watch what moves.
- There is no calculate button. Every figure recalculates as you type or drag, which is what makes this usable for a what-if sweep rather than a single answer.
- Read Tear to Tensile Ratio in the dark results panel — that is the headline figure, expressed in %.
- Check the supporting rows underneath (Tear Index, Tensile per Unit Weight, Tear per Unit Weight and Margin over Minimum) before acting on the headline — they are where an implausible input usually shows itself first.
- Reset to defaults returns every field to the reference case, which is the quickest way to check whether a surprising result came from the tool or from an input you had changed earlier.
Where this is used
- Process planning — establishing Tear to Tensile Ratio before a trial is booked, so machine time and material in Textile Testing & Quality Control are committed against a calculated figure rather than an estimate.
- Costing and quotation — Tear to Tensile Ratio is an input to the cost sheet, and quoting from a worked number rather than a remembered one is what keeps a margin intact.
- Troubleshooting — when the floor result drifts from plan, entering the measured values (starting with Tensile Breaking Strength) shows how much of the gap in Tear to Tensile Ratio each variable explains.
- Teaching and study — the accepted ranges bracket normal Textile Testing & Quality Control practice, so moving one variable at a time shows the shape of the relationship rather than a single answer.
Assumptions and limits
- Tear strength depends on yarn mobility. Resin finishing and very high sett both lock yarns in place and cut tear strength sharply while tensile barely moves.
- Every input is bounded to the range normal practice occupies (Tensile Breaking Strength 1 to 10000 N, Tear Strength 0.1 to 1000 N and Fabric Weight 10 to 1000 g/m², and so on for the rest). Those bounds are guard rails against typing errors, not a claim that the formula fails one unit outside them.
- The calculation is deterministic: the same inputs always give the same result. It carries no allowance for machine condition, operator skill, ambient conditions or lot-to-lot material variation unless an input above explicitly represents one.
- Nothing is sent anywhere. The maths runs in your browser, so the numbers you type never leave the page.
Questions people ask
What do I need to know before using the Tear to Tensile Strength Ratio Calculator?
Have these to hand: Tensile Breaking Strength, Tear Strength, Fabric Weight and Minimum Tear/Tensile Ratio. With those entered, the tool returns Tear to Tensile Ratio immediately.
What exactly is Tear to Tensile Ratio?
Tear strength as a share of tensile strength. It is reported in %. It is derived from Tensile Breaking Strength, Tear Strength, Fabric Weight and Minimum Tear/Tensile Ratio, and is the figure the rest of the Textile Testing & Quality Control calculation is built around.
Which units does this calculator expect?
Enter Tensile Breaking Strength in N, Tear Strength in N, Fabric Weight in g/m² and Minimum Tear/Tensile Ratio in %. Mixing unit systems is the most common cause of a result that looks an order of magnitude wrong — convert before typing, not after reading.
What are the other figures under the main result?
They are the intermediate quantities the calculation passes through: Tear Index, Tensile per Unit Weight, Tear per Unit Weight and Margin over Minimum. They are shown because a headline number nobody can trace is a number nobody trusts — checking them against your own expectation is the fastest way to confirm the inputs were read as you intended.
Can I rely on this for a production decision?
Tear strength depends on yarn mobility. Resin finishing and very high sett both lock yarns in place and cut tear strength sharply while tensile barely moves. Treat the output as an engineering estimate that narrows the trial window, not as a substitute for the trial.