Spunlace Wipe Liquid Retention & Release Calculator

Put this calculator on your own site

Paste this where you want the calculator to appear. It works on any site — WordPress, Squarespace, Webflow, Ghost or plain HTML — and needs no JavaScript of yours. It carries a link back here, which is the only thing we ask for it.

See what it looks like

A wipe has to hold its lotion in the pack and let it go on the surface. Retention and release are the same property pulling in two directions.

Wipe Weights
g
g
Performance Limits
g/g

Retention above which the pack weeps.

g

Liquid Retention Capacity

— g/g

Liquid held per gram of dry substrate

Load & Release

Liquid Absorbed
— g
Lotion Add-on
— %
Margin Below Drip Threshold
— g/g
Liquid Released
— %
Liquid Retained After Release
— g

A negative drip margin means the pack will weep in transit and the bottom wipes will be dry. Release depends on the pressure applied and the surface being wiped, so measure it under a load representative of actual use rather than free drainage — and for a disinfectant wipe, confirm the released volume still delivers the registered dose of active.

Using this calculator

About the Spunlace Wipe Liquid Retention & Release Calculator

The formula

This is the expression the tool evaluates. Every term is named underneath, with the unit it must be supplied in.

Liquid retention capacity, g of liquid per g of dry wipe
lrc = (wetWeight - dryWeight) / dryWeight

Lotion add-on is the same ratio as a percentage.

How far the loading sits below the point where the pack weeps
dripMargin = dripThreshold - lrc

The drip threshold is measured for each substrate and lotion, by loading wipes until free liquid collects in the pack.

Share of the lotion that reaches the surface under load
releaseRatio = rewetMass / (wetWeight - dryWeight) x 100
Symbols used above
SymbolStands forUnit
dryWeightDry Wipe Weightg
wetWeightWet Wipe Weightg
dripThresholdDrip Thresholdg/g
rewetMassLiquid Released Under Loadg
lrcLiquid Retention Capacityg/g
absorbedLiquidLiquid Absorbedg
addOnPercentLotion Add-on%
dripMarginMargin Below Drip Thresholdg/g
releaseRatioLiquid Released%
retainedLiquidLiquid Retained After Releaseg

How the result is derived

Step by step, from the values you type to the figure on screen.

  1. The 4 inputs are read from the form on every keystroke: Dry Wipe Weight, Wet Wipe Weight, Drip Threshold and Liquid Released Under Load.
  2. Each value is checked against the accepted range in the input table below. A value outside its range stops the calculation rather than producing a misleading figure — the results blank out and a message appears.
  3. The validated values are substituted into the expression above, which resolves Liquid Retention Capacity together with every supporting figure in one pass — no value is carried over from a previous entry.
  4. The supporting outputs — Liquid Absorbed, Lotion Add-on, Margin Below Drip Threshold, Liquid Released and Liquid Retained After Release — come from the same pass, so they always describe the same case as the headline figure.
  5. Results are rounded for display only. The full-precision value is used throughout the chain, so reading a rounded intermediate figure back into the tool by hand can shift the last digit.

What each input means

Where to read each value on the floor, the unit it must be in, and the range the tool accepts.

InputUnitAccepted rangeDefaultWhat it means
Dry Wipe Weightg0.1 to 50 g3.2
Wet Wipe Weightg0.1 to 200 g12.8
Drip Thresholdg/g0.5 to 15 g/g3.5Retention above which the pack weeps.
Liquid Released Under Loadg0 to 50 g0.9

What the tool returns

The headline figure and every supporting value it is built from.

OutputUnitWhat it tells you
Liquid Retention Capacity (headline result)g/gLiquid held per gram of dry substrate
Liquid Absorbedg
Lotion Add-on%
Margin Below Drip Thresholdg/g
Liquid Released%
Liquid Retained After Releaseg

Worked example

Given

Dry wipe
3.2 g
Wet wipe
12.8 g
Drip threshold
3.5 g/g
Released under load
0.9 g

Substituting

absorbed = 12.8 - 3.2 = 9.6 glrc = 9.6 / 3.2 = 3.0 g/g, a 300 % add-ondripMargin = 3.5 - 3.0 = 0.5 g/greleaseRatio = 0.9 / 9.6 = 9.4 %; retained = 9.6 - 0.9 = 8.7 g

Answer

Retention
3.0 g/g (300% add-on)
Drip margin
0.5 g/g
Released
9.4%
Left in the wipe
8.7 g

How to use it

  1. Work through the input groups in order — Wipe and Performance. The defaults are a realistic case, so you can change one value at a time and watch what moves.
  2. There is no calculate button. Every figure recalculates as you type or drag, which is what makes this usable for a what-if sweep rather than a single answer.
  3. Read Liquid Retention Capacity in the dark results panel — that is the headline figure, expressed in g/g.
  4. Check the supporting rows underneath (Liquid Absorbed, Lotion Add-on, Margin Below Drip Threshold, Liquid Released and Liquid Retained After Release) before acting on the headline — they are where an implausible input usually shows itself first.
  5. Reset to defaults returns every field to the reference case, which is the quickest way to check whether a surprising result came from the tool or from an input you had changed earlier.

Where this is used

  • Process planning — establishing Liquid Retention Capacity before a trial is booked, so machine time and material in Medical, Hygiene & Barrier Textiles are committed against a calculated figure rather than an estimate.
  • Costing and quotation — Liquid Retention Capacity is an input to the cost sheet, and quoting from a worked number rather than a remembered one is what keeps a margin intact.
  • Troubleshooting — when the floor result drifts from plan, entering the measured values (starting with Dry Wipe Weight) shows how much of the gap in Liquid Retention Capacity each variable explains.
  • Teaching and study — the accepted ranges bracket normal Medical, Hygiene & Barrier Textiles practice, so moving one variable at a time shows the shape of the relationship rather than a single answer.

Reading the result

Typical bands and what each one is telling you.

ValueWhat it indicates
Drip margin negativeOverloaded. Lotion drains to the bottom of the pack: the top wipes dry out and the bottom ones weep. Reduce the add-on or use a more retentive substrate.
Drip margin small but positiveHolds on the bench, but pack temperature, storage time and stacking pressure can push it over. Test packs stored on edge and on their face.
Low release ratioThe substrate holds the lotion too well. Most of what was loaded is thrown away with the used wipe, so a lower add-on may do the same job.

Assumptions and limits

  • A negative drip margin means the pack will weep in transit and the bottom wipes will be dry. Release depends on the pressure applied and the surface being wiped, so measure it under a load representative of actual use rather than free drainage — and for a disinfectant wipe, confirm the released volume still delivers the registered dose of active.
  • Every input is bounded to the range normal practice occupies (Dry Wipe Weight 0.1 to 50 g, Wet Wipe Weight 0.1 to 200 g and Drip Threshold 0.5 to 15 g/g, and so on for the rest). Those bounds are guard rails against typing errors, not a claim that the formula fails one unit outside them.
  • The calculation is deterministic: the same inputs always give the same result. It carries no allowance for machine condition, operator skill, ambient conditions or lot-to-lot material variation unless an input above explicitly represents one.
  • Nothing is sent anywhere. The maths runs in your browser, so the numbers you type never leave the page.

Standards and further reading

  • ISO 9073-6, test methods for nonwovens: absorption, for the liquid absorption capacity of the dry substrate.
  • ISO 9073-1, mass per unit area, which with the wipe size gives the dry wipe weight.

Questions people ask

Is retention capacity the same as the substrate's absorbency?

No. Absorbency is the most the dry substrate can take up in a test. Retention here is what the wipe holds as loaded in the pack, which is set below the absorbency so the pack does not weep.

How should I measure the liquid released under load?

Press the wet wipe onto a weighed blotter or the target surface with a fixed weight for a fixed time, and weigh what transferred. Keep the load and surface the same between samples, since release depends on both.

Why does the substrate change the drip threshold?

Fibre type, blend and web structure set how strongly liquid is held in the pores. A substrate with finer, more wettable fibres holds more lotion before free liquid appears.

Scroll to Top

Follow on WhatsApp

Scan with your phone’s camera to open the channel, then tap Follow.

QR code for the WhatsApp channelOr open WhatsApp on this device