Atlas Material Testing Technology Xenotest 220 is a fabric testing instrument, still in its builder’s current range. Its builder lists samples tested simultaneously up to 250 samples, exposure area 2310 cm2 and chamber temperature up to 65 °C. Fabric testing instruments measure fabric properties such as tensile and tear strength, abrasion and pilling resistance, colour fastness, dimensional stability and air permeability.

Fabric testingTesting and laboratoryIn the builder's current range

Specification

ParameterValue
Test performedISO 105-B02, AATCC TM16 (option 3), M&S C9, C9A
Samples tested simultaneouslyup to 250 samples
Lamp1x 2200 W air-cooled Xenon Lamp
Exposure area2310 cm2
Chamber temperatureup to 65 °C
Black Standard Temperatureup to 100 °C
Specimen holders19 sample holders with capacity for 38 standard textile samples
Water reservoir60l
Stored user-defined tests10

Read from the builder's published page: www.atlas-mts.com, on 2026-11-16.

Check against the machine before you buy or budget on it. Builders publish a range and a configuration; the machine on your floor may be a different variant, may have been rebuilt, and may not carry the options these figures assume. This register records what the builder published, not what any individual machine does.

The record

Read from
www.atlas-mts.com,
Checked by
Textile School,
Last changed

All machinery specifications

Related machines

Report incorrect information on this page

Tell us what is wrong and we will check it against the source. Reports are private, are never published, and go to an editor rather than into a comment thread.

Scroll to Top

Follow on WhatsApp

Scan with your phone’s camera to open the channel, then tap Follow.

QR code for the WhatsApp channelOr open WhatsApp on this device