Branca Idealair Air permeability 37S is a fabric testing instrument, still in its builder’s current range. Its builder lists net weight 30 kg, permeability measuring range 1.4 to 8056 mm/s and pressure drop 0–900 / 0–90 (standard). Fabric testing instruments measure fabric properties such as tensile and tear strength, abrasion and pilling resistance, colour fastness, dimensional stability and air permeability.
Fabric testingTesting and laboratoryIn the builder's current range
Key specifications
Specifications incomplete: 0 of 5 key figures recorded
- Test performed—
- Measuring range—
- Test stations / specimen holders—
- Test standards—
- Specimen size—
- Weight30 kg
Specification
| Parameter | Value |
|---|---|
| Permeability measuring range (Integrale) | 1.4 to 8056 mm/s |
| Pressure drop, standard (Pa / mm H2O) | 0–900 / 0–90 |
| Pressure drop, special (Pa, mm H2O) | 0–2500 Pa, 0–250 mm.H2O |
| Test area as supplied | 100 cm2 |
| Test area reducers | 50 cm2; 20 cm2; 10 cm2; 5 cm2; 2 cm2 |
| Flow meter minimum | 50 l/h, 0,84 l/min |
| Flow meter maximum | 5800 l/h, 96,6 l/min |
| Power supply | 230VAC/50HZ, 110VAC/60HZ |
| Net weight | 30 kg |
Read from the builder's published page: www.brancaidealair.it, on 2026-11-16.
Check against the machine before you buy or budget on it. Builders publish a range and a configuration; the machine on your floor may be a different variant, may have been rebuilt, and may not carry the options these figures assume. This register records what the builder published, not what any individual machine does.
The record
- Read from
- www.brancaidealair.it,
- Checked by
- Textile School,
- Last changed
Related machines
Also from Branca Idealair
Other machines of this kind: Fabric testing
Report incorrect information on this page
Tell us what is wrong and we will check it against the source. Reports are private, are never published, and go to an editor rather than into a comment thread.