Gester Instruments GT-D22 is a laboratory dyeing and finishing machine used in garment laundry and wet finishing, still in its builder’s current range. Its builder lists temperature range 20 - 140 ℃ and heating rate 0.1℃ ~ 9.9℃/ min. It reproduces production dyeing, washing or finishing at small scale, in several beakers or a small drum, to develop recipes and match shades before bulk processing.
Laboratory dyeing and finishing machineLaundry and wet finishing of garmentsIn the builder's current range
Key specifications
3 of 4 key figures recorded
Specification
| Parameter | Value |
|---|---|
| Staining cup number | 12 | 24 |
| Temperature range | 20 - 140 ℃ |
| Heating rate | 0.1℃ ~ 9.9℃/ min |
| Liquor ratio | 1:5 -1: 30 |
| Cooling method | Forced air convection cooling |
| Control mode | 100 programmable steps per process |
| Heat method | Electric heating, infrared tube heating for cup cage/dye cups; low power, small temp difference, no glycerin loss |
| Electric heating power | infrared lamps 6 × 1000 W, 2 tubes in series 5.25 kW |
| Temperature control accuracy | ±0.2 ℃ |
Read from the builder's published page: www.gester-instruments.com, on 2026-11-16.
Check against the machine before you buy or budget on it. Builders publish a range and a configuration; the machine on your floor may be a different variant, may have been rebuilt, and may not carry the options these figures assume. This register records what the builder published, not what any individual machine does.
The record
- Read from
- www.gester-instruments.com,
- Checked by
- Textile School,
- Last changed
Related machines
Also from Gester Instruments
Other machines of this kind: Laboratory dyeing and finishing machine
Elsewhere in Laundry and wet finishing of garments
Report incorrect information on this page
Tell us what is wrong and we will check it against the source. Reports are private, are never published, and go to an editor rather than into a comment thread.