Presto Stantest PTT-560 Prima is a fabric testing instrument, still in its builder’s current range. Its builder lists force for pendulum 1600, 3200 & 6400 gm force, unit scale range 0 -100% and slit size 20 mm. Fabric testing instruments measure fabric properties such as tensile and tear strength, abrasion and pilling resistance, colour fastness, dimensional stability and air permeability.
Fabric testingTesting and laboratoryIn the builder's current range
Key specifications
Specifications incomplete: 1 of 5 key figures recorded
- Test performed—
- Measuring range—
- Test stations / specimen holders—
- Test standardsASTM D1424-09(2013), ASTM D689, ASTM D1922, TAPPI T414
- Specimen size—
Specification
| Parameter | Value |
|---|---|
| Force for Pendulum | 1600, 3200 & 6400 gm force |
| Unit Scale range | 0 -100% |
| Slit Size | 20 mm |
| Calibration Check weight | At 1600gf, at 3200gf, at 6400gf |
| Standards | ASTM D1424-09(2013), ASTM D689, ASTM D1922, TAPPI T414 |
Read from the builder's published page: www.prestogroup.com, on 2026-11-16.
Check against the machine before you buy or budget on it. Builders publish a range and a configuration; the machine on your floor may be a different variant, may have been rebuilt, and may not carry the options these figures assume. This register records what the builder published, not what any individual machine does.
The record
- Read from
- www.prestogroup.com,
- Checked by
- Textile School,
- Last changed
Related machines
Also from Presto Stantest
Other machines of this kind: Fabric testing
Report incorrect information on this page
Tell us what is wrong and we will check it against the source. Reports are private, are never published, and go to an editor rather than into a comment thread.