Roaches International Opti-Air is a fabric testing instrument, still in its builder’s current range. Its builder lists weight 125kg, pressure range 1 – 1,000Pa and measuring range 0.2 – 12,000mm/s. Fabric testing instruments measure fabric properties such as tensile and tear strength, abrasion and pilling resistance, colour fastness, dimensional stability and air permeability.
Fabric testingTesting and laboratoryIn the builder's current range
Key specifications
4 of 5 key figures recorded
- Make
- Roaches InternationalUnited Kingdomroaches.co.uk (the builder's website, opens in a new tab) All 34 machines from Roaches International
- Class
- Fabric testing
- Process stage
- Testing and laboratory
- Lifecycle
- In the builder's current range
Specification
| Parameter | Value |
|---|---|
| Test performed | Air permeability |
| Pressure Range | 1 – 1,000Pa |
| Measuring Range | 0.2 – 12,000mm/s |
| Measuring Accuracy | ±2% |
| Sample Thickness (Max) | 12mm |
| Test Heads | 3 Supplied as standard: 5cm², 20cm², 25cm², 38cm², 50cm², 100cm² (Please specify) |
| Orifice Plate | 1pc with 8 different apetures |
| Power Supply | 220V, 50Hz, 1 Phase |
| Dimensions | 850 x 520 x 1050mm |
| Weight | 125kg |
| Standards | ASTM D737, ASTM D5636, BS5636, DIN 53887, EN ISO 7231, EN ISO 9237 |
Read from the builder's published page: www.roaches.co.uk, on 2026-11-16.
Check against the machine before you buy or budget on it. Builders publish a range and a configuration; the machine on your floor may be a different variant, may have been rebuilt, and may not carry the options these figures assume. This register records what the builder published, not what any individual machine does.
The record
- Read from
- www.roaches.co.uk,
- Checked by
- Textile School,
- Last changed
Related machines
Also from Roaches International
Other machines of this kind: Fabric testing
Report incorrect information on this page
Tell us what is wrong and we will check it against the source. Reports are private, are never published, and go to an editor rather than into a comment thread.