Home » Regulations » US Carpet Flammability (FF 1-70) — 16 CFR Part 1630

US Carpet Flammability (FF 1-70) — 16 CFR Part 1630

Checked by an editor

US Carpet Flammability (FF 1-70) — 16 CFR Part 1630

Citation
16 CFR Part 1630
Jurisdiction
US
Made by
Consumer Product Safety Commission
Instrument
Regulation
Status
In force

What it requires (2 obligations)

This Standard applies to all types of carpets and rugs used as floor covering materials, regardless of method of fabrication and whether made of natural or synthetic fibers or films, combinations of these or substitutes for them. A specimen passes if the charred portion does not extend to within 2.54 cm (1.0 in) of the edge of the hole in the flattening frame at any point, and at least seven of the eight specimens must meet that criterion for the product to conform.

No date set Confirmed In force, dates fixed in published law

Who it falls on
Manufacturers, importers and sellers
Products
Carpets, floor coverings, home textiles, textiles
Markets
US

Fibre-neutral by construction: the scope names natural fibres, synthetic fibres, films, combinations and substitutes, so the material cannot put a floor covering outside the Standard. One-of-a-kind items such as an antique, an Oriental or a hide may be excluded under conditions established by the Commission.

Quoted from 16 CFR §§ 1630.2(a), 1630.3(b) test criterion and 1630.3(c) acceptance criterion, eCFR snapshot 2026-08-01.

A carpet or rug is within this Standard where it has one dimension greater than 1.83 m (6 ft) and a surface area greater than 2.23 m² (24 sq ft). Products such as carpet squares with one dimension less than 1.83 m and a surface area less than 2.23 m², but intended to be assembled on installation into assemblies that may exceed those figures, are INCLUDED in this definition.

No date set Confirmed In force, dates fixed in published law

Who it falls on
Manufacturers, importers and sellers
Products
Carpets, floor coverings, home textiles, textiles
Markets
US

Carpet squares are the trap. The tile in a manufacturer's hand is small; the assembly it is designed to become is large, and this Part follows the assembly. The companion small-carpet Standard at Part 1631 excludes them expressly and sends them here, so measuring the product as supplied reaches the wrong Part. The test method and both criteria are identical to the companion Standard: a specimen passes if the charred portion does not extend to within 2.54 cm (1.0 in) of the edge of the hole in the flattening frame, and at least seven of eight specimens must pass. Which Part applies changes the certification, not the performance required.

Quoted from the definition of "carpet or rug" in § 1630.1, including the carpet-squares sentence.

Read the official text

This is a register, not advice. It records what an instrument says and when it applies. Whether it applies to a particular company, product or shipment is a question for somebody who knows that business, and the answer is frequently not what the summary above would suggest.

The compliance calendar

Every regulation in the United States · Home Textile regulations · Carpet & Rug regulations

Report incorrect information on this page

Tell us what is wrong and we will check it against the source. Reports are private, are never published, and go to an editor rather than into a comment thread.

Scroll to Top

Follow on WhatsApp

Scan with your phone’s camera to open the channel, then tap Follow.

QR code for the WhatsApp channelOr open WhatsApp on this device