Home » Standards » ASTM » Page 47

Standards crosswalk

ASTM

ASTM appears on 528 crosswalks here — as the issuing body, or as an equivalent to another body's standard.

Any body’s number. It lands on the crosswalk that covers it, whichever body issued it.

Every issuing body

Showing 461–470 of 528 Show the whole register

ASTM International

Test methods and specifications across materials; textiles are committee D13. Frequently named in North American buyer specifications.

United States, widely cited elsewhere Official site

What are ISO, ASTM and AATCC — and what do IDT, MOD and NEQ mean?

Calculators on this site cite 35 further standards that the register does not cover yet. They are being written in order of how many tools need them.

ASTM D7983

Standard Test Method for Shrinkage of Carpet Backing Fabrics

Standard Test Method for Shrinkage of Carpet Backing Fabrics

ASTM D7984

Standard Test Method for Measurement of Thermal Effusivity of Fabrics Using a Modified Transient Plane Source (MTPS) Instrument

Standard Test Method for Measurement of Thermal Effusivity of Fabrics Using a Modified Transient Plane Source (MTPS) Instrument

ASTM D8007

Standard Test Method for Wale and Course Count of Weft Knitted Fabrics

Standard Test Method for Wale and Course Count of Weft Knitted Fabrics

ASTM D8041/D8041M

Standard Test Method for Whole Boot Breathability (MVTR)

Classified under ICS 13.340.50 Leg and foot protection. Covers the finished article rather than the fibre or fabric it is made from, which is what separates this class…

ASTM D8171

Standard Test Methods for Density Determination of Flax Fiber

Standard Test Methods for Density Determination of Flax Fiber

ASTM D8248

Standard Terminology for Smart Textiles

Standard Terminology for Smart Textiles

ASTM D8289

Standard Test Method for Tensile Strength Estimate by Disc Compression of Manufactured Graphite

Classified under ICS 59, the international subject classification for textile and leather technology.

ASTM D8337/D8337M

Standard Test Method for Evaluation of Bond Properties of FRP Composite Applied to Concrete Substrate using Single-Lap Shear T

Classified under ICS 59, the international subject classification for textile and leather technology.

ASTM D8342/D8342M

Standard Test Method for Measuring the Probability of a Full Length Burn on a Cannabis/Hemp Pre-roll

Classified under ICS 97.160 Home textiles and linen. Covers the finished article rather than the fibre or fabric it is made from, which is what separates this class…

ASTM D8394

Standard Test Method for Automated Measurement of Maturity, Fineness, Ribbon Width, and Micronaire of Cotton Fibers

Standard Test Method for Automated Measurement of Maturity, Fineness, Ribbon Width, and Micronaire of Cotton Fibers