AS/NZS
AS/NZS 4547.5
Methods of testing woolpacks for greasy wool - Part 5: Strength of fabric after exposure to ultraviolet radiation
Methods of testing woolpacks for greasy wool - Part 5: Strength of fabric after exposure to ultraviolet radiation
Reference register
3,130 test methods indexed by number across ISO, ASTM, AATCC, BIS, GB, JIS and EN, 539 of them with a full record. Where an equivalent is known it is stated as IDT, MOD or NEQ, with the deviation declared wherever it is MOD.
AATCC (5) · amfori (1) · AS/NZS (62) · ASTM (532) · Better Cotton (2) · BIS (313) · bluesign (4) · BS (212) · C2C (3) · CEN (411) · DD (1) · EDANA/INDA (1) · EN (1) · Fairtrade (1) · GOTS (6) · Higg Index (5) · IEC (7) · ISEAL (4) · ISO (1,359) · ISO/IEC (7) · ISO/TR (2) · ISO/TS (3) · LWG (4) · NZS (6) · OEKO-TEX (8) · PAS (1) · PD (4) · SA8000 (1) · SAC (458) · SLCP (1) · Textile Exchange (9) · WRAP (1) · ZDHC (6)
Showing 591–600 of 3,130
What are ISO, ASTM and AATCC — and what do IDT, MOD and NEQ mean?
Calculators on this site cite 88 further standards that the register does not cover yet. They are being written in order of how many tools need them.
AS/NZS
Methods of testing woolpacks for greasy wool - Part 5: Strength of fabric after exposure to ultraviolet radiation
Methods of testing woolpacks for greasy wool - Part 5: Strength of fabric after exposure to ultraviolet radiation
AS/NZS
High visibility safety garments - Part 1: Garments for high risk applications
High visibility safety garments - Part 1: Garments for high risk applications
AS/NZS
High visibility safety garments - Part 2: Garments for fire service personnel
High visibility safety garments - Part 2: Garments for fire service personnel
AS/NZS
Protective clothing for firefighters - Laboratory test methods and performance requirements for wildland firefighting clothing
Protective clothing for firefighters - Laboratory test methods and performance requirements for wildland firefighting clothing
AS/NZS
Protective clothing for firefighters - Requirements and test methods for protective clothing used for structural firefighting
Protective clothing for firefighters - Requirements and test methods for protective clothing used for structural firefighting
ASTM
Standard Specification for Fabrication of Flexible Removable and Reusable Blanket Insulation for Hot Service
Classified under ICS 13.340.99 Other protective equipment. Covers the finished article rather than the fibre or fabric it is made from, which is what separates this class from…
ASTM
Standard Test Method for Yarn Number Based on Short-Length Specimens
Standard Test Method for Yarn Number Based on Short-Length Specimens
ASTM
Standard Test Method for Vegetable Matter and Other Alkali-Insoluble Impurities in Scoured Wool
Standard Test Method for Vegetable Matter and Other Alkali-Insoluble Impurities in Scoured Wool
ASTM
Standard Test Method of Sampling and Testing Staple Length of Grease Wool
Standard Test Method of Sampling and Testing Staple Length of Grease Wool
Every record in these registers was sent in by somebody. Submissions are reviewed before they are published.
4,262 machines in the register.Tell us about a missing one 806 event series in the register.Submit a trade fair or conference 3,130 standards tracked in the register.Get the changes by email each week