Acrylic Fibers

Acrylic fibres are polymers formed by addition polymerization of at least 85% by weight of a chemical called acrylonitrile or vinyl chanide. To polymerise vinyl cyanide the double bond between the first two carbon atoms is broken and the…
Read More...

Synthetic Fibers

The synthetic man-made fibers include the polyamides (nylon), polyesters, acrylics, polyolefin, vinyl, and elastomeric fibers, while the regenerated fibers include rayon, the cellulose acetates, the regenerated proteins, glass and rubber…