Grams per Meter 0.5905 / Ne
Grams per Yard 0.54 / Ne
Tex den x .11 = 1000/Nm = Mic/25.4
Ne Nm/1.693
DRAFT (feed weight in g/m) / (delivery weight in g/m)
DRAFT Tex (feed)/Tex(delivery)
DRAFT delivery roll surface speed/feed roll surface speed
No. of hanks delivered by m/c (Length delivered in m/min)/1.605grams per meter = 0.5905/Ne

Carding

Production in kgs / hr ( L x 1.0936 x 60 x effy ) / (hank (Ne) x 36 x 840 x 2.2045)

L – delivery speed in m/min
effy- efficiency
Ne – English count ( number of 840 yards in one pound)
840 – constant
2.2045- to convert from lbs to kilograms

Production in kgs / hr (L x Ktex x 60 x effy) / ( 1000 )

L – delivery speed in m/min
Ktex- sliver count in Ktex (kilotex)
effy – efficiency
1000- to convert to kilograms from grams

Production in kgs / 8 hrs (0.2836 x L x effy) / (Ne)

L – delivery speed in m/min
effy – efficiency
Ne – English count

Production / 8 hrs (Hank x Nd) /( Ne x 2.2045)

Hank = no of hank (840 yards)delivered by the machine
Nd = no of deliveries
Ne = hank of the material

Total draft in card (feed weight in g/m) / (sliver weight in g/m)

Drawframe

Break draft surface speed of 2nd roller / surface speed of back roller
Main draft surface speed of 1st roller / surface speed of 2nd( middle) roller
Total draft surface speed of delivery roller / surface of feed roller
Production in kgs / 8 hrs (0.2836 x L x effy x Nd) / (Ne)

L – delivery speed in m/min
effy – efficiency
Ne – english count
Nd – No of delvieries

Production in kgs / hr (FRD x FRrpm x 3.14 x 60 x effy x Nd) / (Ne x 840 x 36 x 2.2045)

FRD – front roller dia in inches
FRrpm – front roller rpm
effy – efficiency
Ne – Sliver hank
Nd – number of deliveries

Speedframe & Ringframe

Twist / Inch (TPI) Spindle speed / FRS

FRS – front roller surface speed in inches/mi

FRS = FRrpm x 3.14 x FRD FRS – Front roller surface speed

FRD – front roller diamete

T.P.I T.M. x sqrt(count or hank)

T.M. – Twist multiplier
sqrt – square root

Production in kgs / 8 hrs (7.2 x SS x effy) / (TPI x Ne x 1000)

SS – spindle speed

Spindle speed m/min x TPI x 39.37
Hank delivered spindle speed / ( tpi x 62.89)
Ring traveller speed in m/sec (spindle speed x ring dia in mm x 3.14) / (60 x 1000)

Winding

Production in kgs / 8 hrs (0.2836 x L x effy x Nd) / (Ne)

L – delivery speed in m/min
effy – efficiency
Ne – english count
Nd – No of delvieries

Production in kgs / hr ( L x 1.0936 x 60 x effy ) / (hank (Ne) x 36 x 840 x 2.2045)

L – delivery speed in m/min
effy- efficiency
Ne – English count ( number of 840 yards in one pound)
840 – constant
2.2045- to convert from lbs to kilograms

22 Comments
  1. PAYAL KANARA says

    WHEN I GET DIFFERENCE BETWEEN FR SPEED BY TACHOMETER AND TO MACHINE DISPLAY THAN WHAT A PROBLEM I SUFFER IN MY MACHINE.
    IS IT BY MECHANICAL SIDE OR ELECTRICAL SIDE?
    EX. IN TACHOMETER FR SPEED IS 280
    IN MACHINE DISPLAYED FR SPEED 250.

  2. Waqas Ali says

    Ring Frame Ry4 ki front roller se spindle speed kesy nikaly geyn ??

  3. Suresh says

    The constant 3.14 how to create?

  4. shrihari vinayak deshpande says

    Sir,
    Im very new to spinning and also unknown person to spinning. but due to covid 19 ,im joining spinning unit . as supervisor. plz let me know the formulaes.

  5. SANKARSAN BEHERA says

    R/SIR. HOW CALCULATE THE REWIDING BREKS IN AUTO CONER ANY ENGLISH COUNT.

  6. Harikrishnan.S says

    In prodn calculation you have multiply the Ss with 7.2,what is this,how it is derived pl explain

    1. VASANT BHANDARY says

      Production :
      Grams/Spdl/Shift
      = 7.2 * Spdl. Speed/TPI * Count
      Where 7.2
      = 8 * 60 * 1000 * 1.0936/840 * 39.37 * 2.2046

  7. Raju says

    How to calculate average speed(spinnin)?

  8. irshad says

    im a investigator in rnd rnd formula all pls

  9. Sanjay Prajapati says

    dear sir,

    I am training supervisor in the textile industry spinning plant, so plz tell me calculation ring frame, auto corner, cheese winding and (TFO) with calculation formula

  10. Jayaraj says

    It is base value
    If one 840 yard yarn weighs one pound it will one count
    Similarly if one pound of yarn give 840 yards of 49 times it will be 40 s count ne

  11. Raja Haider Ali Bhatti says

    36 in the calculation is wrong as you are converting meters into yards already by multiplying meters/m with 1.09.

    1. pawan says

      yes absolutely right… you are

  12. Dharam chand says

    Why 840 Yard constant in textile

    1. Pat says

      That is the question!. That is how someone was able to order the same weight of yarn agai and n!

      I believe that was as much as a bobbin held back then, so it was a standard measurement. No one understands why!!

      So if you were able tp get 16 hanks out of a pound, it was said to be “16 weight”, or size 16, That weight of yarn was a way for a customer to order the same weight of yarn again. Which is why we have 8 and 16 and 24 weight of yarns today.

      Unfortunately, this doesn’t apply the same to all fibers — each has its own standard measurement.

      At least, it seems plausible to me!

  13. Zoauddin says

    Dear Sir
    I want and I you about profit and cost.

    Pls can you explains me about quality formulas example (60×60×40)/(60×60×40)=61
    Pls explain me?

    If I know what quality I want use on looms how can I know production cost?

    Best regards

    1. Sanjay Prajapati says

      dear sir,

      I am training supervisor in the textile industry spinning plant, so plz tell me calculation ring frame, auto corner, cheese winding and (TFO) with calculation formula

  14. NAVEEN KUMAR GURRAM says

    how to increase noil percentage in comber e65 reiter

    what is meant by propack in autoconer aerlicon

  15. Gajanand Bihani says

    how to calculate TM for double yarn, say 2/60 cotton yarn.

  16. V.S. Shekhawat says

    Carding gauge in pv yarn

    1. Muhammad Esmaeel says

      card Engeenir Muhammad esmaeel
      Email
      Yasiresmaeel@yahoo.com

  17. gopal says

    wat is T.M explain twist multiplier

Leave A Reply

Your email address will not be published.