Characteristics of Rayon Fiber
Rayon is moisture absorbent (more so than cotton), breathable, comfortable to wear, and easily dyed in vivid colors. It does not build up static electricity, nor will it pill unless the fabric is made from short, low-twist yarns.
Rayon Fiber’s cellulosic base contributes many properties similar to those of cotton or other natural cellulosic fibers. Rayon Fiber is comfortable, soft to the skin, and has the moderate dry strength and abrasion resistance.
One of the Rayon Fiber’s strengths is its versatility and ability to blend easily with many fibers—sometimes to reduce cost, other times for luster, softness, or absorbency and resulting comfort. HWM rayons readily take finishes such as mercerization, sanforization (shrink resistance), and permanent press.
Rayon is probably the most misunderstood of all fibers. It is not a natural fiber, yet it is not synthetic. It is a fiber formed by regenerating natural materials into a usable form.
Peculiar Characteristics
Rayon has moderate resistance to acids and alkalis and generally the fiber itself is not damaged by bleaches; however, dyes used in the fabric may experience a color change. As a cellulosic fiber, rayon will burn, but flame retardant finishes can be applied.
Like other cellulosic fibers, it is not resilient, which means that it will wrinkle. Rayon withstands ironing temperatures slightly less than those of cotton. It may be attacked by silverfish and termites, but generally resists insect damage. It will mildew, but that generally is not a problem.
Consumers should be aware of several cautions in relation to proper use and care of fabrics made from rayon fiber. Regular or viscose rayon has low wet strength, resulting in loss of stability or the tendency to shrink or stretch easily when wet. Although resin-treated rayons can sometimes be hand or machine washed with success, regular rayon normally requires dry cleaning to maintain appearance and shape.
There is a finish that can be applied to make viscose rayon fabrics washable and limit shrinkage to 3 percent. It is formaldehyde-free and will not affect the hand, width, or length of treated fabrics. It can be used on challis, families, and other fabrics that otherwise would require dry cleaning to maintain appearance.
Consumers should also note that HWM or polynosic rayon has high wet strength. Fabrics made from this fiber can usually be machine washed and tumble dried. Polynosic rayon functions and handles during use and care similarly to cotton. Unfortunately, it is often difficult to identify whether a garment is made from polynosic or viscose rayon unless identified on the label. Read labels, look for trade names, and follow care recommendations.
In some instances, polynosic or HWM rayons may be “low labeled.” This means that manufacturers have recommended dry cleaning when hand washing or machine washing would be satisfactory. Sometimes the fabric may be washable, but trims, linings, or other aspects of the garment may not be. Unfortunately, consumers take a risk when they care for a rayon garment in a manner other than that recommended by the care label.
Moisture-Sensitive Sizing and Dyes
Sizings or starches applied to rayon during finishing give body, sheen, luster, shape, and control relaxation shrinkage. In some instances, they may enhance strength. Unfortunately, some of the sizings and dyes used on rayon are sensitive to moisture.
When moisture contacts them, the sizing or dye migrates to the edge of the wet spot and forms a “ring” on the fabric. Raindrops, splashes from tap water, as well as water-based food substances will form dark rings on these fabrics. The rings may be difficult to remove without submerging the entire garment in water. This process can cause further damage to viscose rayons, which have low wet strength.
The migration of dyes and sizings from moisture further complicates stain removal in dry cleaned garments. Dry cleaning solvents are designed to remove oil-based stains. Water-based stains such as fruit juice and beverages and certain foodstuffs require moisture for stain removal. While this process removes the stain, it may also cause dye or sizing migration in the rayon fabrics, leaving a water spot ring.
Also, as a result of the general dry cleaning process, swirls or waves may occur on the fabric surface. This is caused by a disturbance in the sizing from moisture in steam pressing, compounded by heat and pressure associated with the process. Generally, these surface disturbances cannot be completely removed.
Loss of Body
Rayon fabrics may lose a body or become limp over time from abrasion or general removal of sizing during dry cleaning. Dry cleaners can apply sizings, but they seldom duplicate the effect achieved during commercial processing. Application of sizing also reduces seam slippage, raveling, and fraying of fabrics.
Since the finish is not permanent, it can result in changes in fabrics and their performance, such as loss of body, luster, seam slippage, and raveling. The consumer should note that moisture-sensitive dyes or finishes are generally not applied to polynosic rayons and should not cause problems during use and care of these fabrics.
Also related to sizing application is yellowing of fabrics over time. Some sizings or starches oxidize and yellow with age. The problem is most noticeable in exposed areas such as collars, shoulders, and outside sleeves, especially on white or light-colored fabrics. Wet cleaning, often accompanied by bleaching will correct the problem; however, this treatment may cause additional damage from shrinkage or loss of body.
Other cautions related to rayons are pilling, relaxation shrinkage, and fusing of blends. Short, low-twist fibers, which contribute a soft hand to garments, rub or abrade during wear. These fibers mat together and form fiber balls or pills on the fabric surface. Pills may be “shaved” or clipped off; however, as this is done, fibers are being removed, creating a thinner layer of fabric. The problem is less likely to occur on fabrics with a hard surface and those made from longer, or higher twist yarns.
Rayon fabric is especially susceptible to relaxation shrinkage, which occurs over a period of time from routine laundering or dry cleaning. Consumers should consider this tendency when selecting garments, particularly those that are more fitted.
Because viscose rayon is less stable when wet, uneven hemlines may occur in full bias skirts or dresses made from rayon crepe fabrics. The problem can be especially bothersome in damp climates. Bias hemlines are notorious for stretching and changing length over time, but especially so if garments are made from viscose rayon crepe. Hems in these garments may need to be re-marked and evened-up over time.
Rayon is a versatile fiber and is frequently found in blends with polyester, nylon, and acrylic—all of which are synthetics and heat sensitive. These fibers generally contribute strength, wrinkle resistance, and ease of care to rayon blends. During care, iron temperatures safe for rayon can be too hot, melting or fusing the heat-sensitive synthetic fibers. This process cannot be reversed and results in slits, tears, brittleness in the fabric, or shiny areas.
Caring Rayon Fiber/Fabrics
The critical element in successful care of rayon is the type of fiber. Regular or viscose rayons usually require dry cleaning for best results, while high wet modulus, high wet strength or polynosic rayons, will normally machine wash and tumble dry satisfactorily (see Fiber Types and Cautions sections).
The low wet strength of untreated viscose rayon is likely to cause shrinkage and loss of body if fabrics made from these fibers are hand or machine washed. Viscose rayons are usually labeled “dry clean only.” Check and follow garment labels for care and instructions.
Consumers who do not follow care instructions will have no recourse to manufacturers should damage occur during laundering. Since many dyes and finishes applied to viscose rayon are moisture-sensitive, consumers should protect garments from contact with moisture. Raincoats should be worn on stormy days. Also, care should be used when washing hands or working in the kitchen to avoid splashing water.
The problem with sizing or dye migration increases the longer the area remains damp. Spills or moisture should be blotted with the absorbent cloth to remove moisture. Avoid spilling acid or alkali, such as foodstuffs or perfume, as certain dyes used on rayon are especially sensitive to these substances.
Use caution or avoid treating stained areas with water. Take the garment to a dry cleaner for stain removal. Rings or darker shading caused by sizing migration and lighter areas resulting from dye migration may be permanent.
When viscose rayons can be hand washed, do so with care. Always support wet fabrics, since rayon has a low wet strength and is unstable when wet. Avoid wringing moisture from fabrics. Gently squeeze out moisture and roll in a towel. Smooth and shape, then lay flat to dry. If the garments are not too heavy when wet, they can be hung on a non-rusting hanger.
When pressing regular rayon garments at home, guard against spitting by steam irons that may cause water spots. Also, if possible, press on the wrong side or use a press cloth on the right side to avoid shine or iron imprints. Use a rayon or synthetic setting on the iron. When pressing blends, use the iron temperature for the most heat-sensitive fiber. Normally, a synthetic setting will be satisfactory.
High wet modulus or polynosic rayons can usually be machine washed or dried without special care. Blends, dark colors, and permanent press fabrics should be washed on a gentle cycle with warm water; however, 100 percent high wet modulus rayons are normally not damaged by hot water temperatures (more than 140°F).
Tumble dry on a warm setting and remove immediately, or while slightly damp. Smooth and hang to reduce wrinkling. Polynosic rayons can be line dried; however, heavy items should be supported by clotheslines to avoid stretching or loss of shape.
Summary
Rayon is probably the most misunderstood of all fibers. It is not a natural fiber, yet it is not synthetic. It is a fiber formed by regenerating natural materials into a usable form. As an inexpensive fiber, rayon has often been used in low-end, poorly constructed garments that have tarnished its reputation.
The two major types of rayon, regular viscose, and high wet modulus or polynosic, have created further confusion and contributed to improper care practices by consumers not aware that two fabrics with the same fiber content might require totally different methods of care.
Rayon fibers and fabrics made from them have many desirable properties. However, consumers sometimes expect performance characteristics beyond those for which rayon fibers were designed.
Although rayon can look like wool, silk, cotton, or linen and is a manufactured fiber like polyester, this does not mean it behaves like or has the same properties or care requirements of these fibers. Rayon is a fiber unto itself. Consider each a garment made from rayon individually when determining use and care practices.
I have a question. Would layers and layers of rayon fabric be good for a home made “N95” masks?