Introduction to breathable water-repellent textiles and their production methods

Type of Breathable textile materials | Methods of producing Breathable textiles

1 11,324

Breathability refers to the ability of a fabric to absorb moisture and release it through the material itself, allowing it to ‘breathe’. Breathable Fabrics transmit body moisture away from the body, thus maximizing comfort and dryness during outdoor activities.

How DWRs Work

DWRs work by increasing the “contact angle” or “surface tension” created when water contacts a textile. Basically, a high contact angle creates a microscopically “spiky” surface that suspends water droplets on the outer fringe of the fabric.

breathable-fabrics-contact-angle

An optimized DWR keeps droplets in a rounded shape—like a dome-shaped bead. The rounder the droplet, the easier it rolls off the fabric. A low contact angle permits droplets to assume a flattering shape, one that can spread out like a splotch, cling to the fabric’s surface and eventually seep into it.

DWR Ratings

Manufacturers generally measure DWR effectiveness by a spray test. Water is sprayed onto a textile, and the amount that sticks is visually assessed. A score of 90 points indicated that roughly 90% of the fabric has no water sticking to it. The higher the number, the better the performance. The test is then repeated after a number of washings to determine durability.

Test scores and the number of washings is combined to create a rating. For example, a 90/10 rating means the spray test achieved a total of 90 points after 10 washes.

Not all manufacturers publish DWR performance ratings, but here is a basic guide for interpreting any that you find:

  • Good: 80 points after 10 washes. This is a basic outerwear finish.
  • Excellent: 80 points after 20 washes. Marmot, for example, uses this as its minimum rating for outerwear.
  • Superior: 80 points after 50 to 100 washes.
Pages ( 3 of 7 ): « Previous12 3 45 ... 7Next »
1 Comment
  1. Arjun Murali says

    Thank you for the detailed explanation Mr. Ashok Haboo. It has been very helpful for a new merchandiser like me. I have recently started a textile startup called swagswami.comSwag Swami and we are in the process of developing new breathable activewear for the Indian Market. This article has helped me a lot!

    Thank you once again Sir!

Leave A Reply

Your email address will not be published.