Home » Calculators » Testing & Quality » Textile Testing & Quality Control » Colour Difference Delta E & CMC Acceptability Calculator
Jump to a calculator 671 tools

Testing & Quality Control

Colour Difference Delta E & CMC Acceptability Calculator

Put this calculator on your own site

Paste this where you want the calculator to appear. It works on any site — WordPress, Squarespace, Webflow, Ghost or plain HTML — and needs no JavaScript of yours. It carries a link back here, which is the only thing we ask for it.

See what it looks like

CMC weights lightness, chroma and hue differently because the eye does. Delta E*ab does not.

Standard Reference shade
Batch Production sample
CMC Parameters Commercial setting
dE

Delta E CMC

— dE

Perceptually weighted colour difference

Difference Components

Delta E*ab (CIE 1976)
— dE
Lightness Difference
— dL
Chroma Difference
— dC
Hue Difference
— dH
Margin Inside Tolerance
— dE

CMC(2:1) is the usual textile setting and tolerates lightness shifts twice as readily as chroma shifts. A negative margin means the batch fails.

Using this calculator

About the Colour Difference Delta E & CMC Acceptability Calculator

The formula

This is the expression the tool evaluates. Every term is named underneath, with the unit it must be supplied in.

Delta E CMC
deltaECmc = f( l1, a1, b1, l2, a2, b2, lightness, chroma, tolerance )

Each input feeds the expression evaluated in the browser; the symbol table below names every term and its unit.

Symbols used above
SymbolStands forUnit
l1L* Standard—
a1a* Standard—
b1b* Standard—
l2L* Batch—
a2a* Batch—
b2b* Batch—
lightnessLightness Weight (l)—
chromaChroma Weight (c)—
toleranceCommercial TolerancedE
deltaECmcDelta E CMCdE
deltaEabDelta E*ab (CIE 1976)dE
deltaLLightness DifferencedL
deltaCChroma DifferencedC
deltaHHue DifferencedH
passMarginMargin Inside TolerancedE

How the result is derived

Step by step, from the values you type to the figure on screen.

  1. The 9 inputs are read from the form on every keystroke: L* Standard, a* Standard, b* Standard, L* Batch, a* Batch, b* Batch, Lightness Weight (l), Chroma Weight (c) and Commercial Tolerance.
  2. Each value is checked against the accepted range in the input table below. A value outside its range stops the calculation rather than producing a misleading figure — the results blank out and a message appears.
  3. The validated values are substituted into the expression above, which resolves Delta E CMC together with every supporting figure in one pass — no value is carried over from a previous entry.
  4. The supporting outputs — Delta E*ab (CIE 1976), Lightness Difference, Chroma Difference, Hue Difference and Margin Inside Tolerance — come from the same pass, so they always describe the same case as the headline figure.
  5. Results are rounded for display only. The full-precision value is used throughout the chain, so reading a rounded intermediate figure back into the tool by hand can shift the last digit.

What each input means

Where to read each value on the floor, the unit it must be in, and the range the tool accepts.

InputUnitAccepted rangeDefaultWhat it means
L* Standard—0 to 10050
a* Standard—-128 to 12825
b* Standard—-128 to 128-20
L* Batch—0 to 10051.2
a* Batch—-128 to 12824.1
b* Batch—-128 to 128-19.3
Lightness Weight (l)—0.5 to 52
Chroma Weight (c)—0.5 to 51
Commercial TolerancedE0.1 to 10 dE1

What the tool returns

The headline figure and every supporting value it is built from.

OutputUnitWhat it tells you
Delta E CMC (headline result)dEPerceptually weighted colour difference
Delta E*ab (CIE 1976)dE
Lightness DifferencedL
Chroma DifferencedC
Hue DifferencedH
Margin Inside TolerancedE

Worked example

Given

L* Standard
50
a* Standard
25
b* Standard
-20
L* Batch
51.2
a* Batch
24.1
b* Batch
-19.3
Lightness Weight (l)
2
Chroma Weight (c)
1
Commercial Tolerance
1 dE

The tool loads with this case already solved — the Delta E CMC shown above is its answer. Change one value and the difference from this baseline is the sensitivity of the result to that variable.

How to use it

  1. Work through the input groups in order — Standard, Batch and CMC Parameters. The defaults are a realistic case, so you can change one value at a time and watch what moves.
  2. There is no calculate button. Every figure recalculates as you type or drag, which is what makes this usable for a what-if sweep rather than a single answer.
  3. Read Delta E CMC in the dark results panel — that is the headline figure, expressed in dE.
  4. Check the supporting rows underneath (Delta E*ab (CIE 1976), Lightness Difference, Chroma Difference, Hue Difference and Margin Inside Tolerance) before acting on the headline — they are where an implausible input usually shows itself first.
  5. Reset to defaults returns every field to the reference case, which is the quickest way to check whether a surprising result came from the tool or from an input you had changed earlier.

Where this is used

  • Process planning — establishing Delta E CMC before a trial is booked, so machine time and material in Textile Testing & Quality Control are committed against a calculated figure rather than an estimate.
  • Costing and quotation — Delta E CMC is an input to the cost sheet, and quoting from a worked number rather than a remembered one is what keeps a margin intact.
  • Troubleshooting — when the floor result drifts from plan, entering the measured values (starting with L* Standard) shows how much of the gap in Delta E CMC each variable explains.
  • Teaching and study — the accepted ranges bracket normal Textile Testing & Quality Control practice, so moving one variable at a time shows the shape of the relationship rather than a single answer.

Assumptions and limits

  • CMC(2:1) is the usual textile setting and tolerates lightness shifts twice as readily as chroma shifts. A negative margin means the batch fails.
  • Every input is bounded to the range normal practice occupies (L* Standard 0 to 100, a* Standard -128 to 128 and b* Standard -128 to 128, and so on for the rest). Those bounds are guard rails against typing errors, not a claim that the formula fails one unit outside them.
  • The calculation is deterministic: the same inputs always give the same result. It carries no allowance for machine condition, operator skill, ambient conditions or lot-to-lot material variation unless an input above explicitly represents one.
  • Nothing is sent anywhere. The maths runs in your browser, so the numbers you type never leave the page.

On this site

Articles that explain what this tool calculates.

Questions people ask

What do I need to know before using the Colour Difference Delta E & CMC Acceptability Calculator?

Have these to hand: L* Standard, a* Standard, b* Standard, L* Batch, a* Batch, b* Batch, Lightness Weight (l), Chroma Weight (c) and Commercial Tolerance. With those entered, the tool returns Delta E CMC immediately.

What exactly is Delta E CMC?

Perceptually weighted colour difference. It is reported in dE. It is derived from L* Standard, a* Standard, b* Standard, L* Batch, a* Batch, b* Batch, Lightness Weight (l), Chroma Weight (c) and Commercial Tolerance, and is the figure the rest of the Textile Testing & Quality Control calculation is built around.

Which units does this calculator expect?

Enter Commercial Tolerance in dE. Mixing unit systems is the most common cause of a result that looks an order of magnitude wrong — convert before typing, not after reading.

What are the other figures under the main result?

They are the intermediate quantities the calculation passes through: Delta E*ab (CIE 1976), Lightness Difference, Chroma Difference, Hue Difference and Margin Inside Tolerance. They are shown because a headline number nobody can trace is a number nobody trusts — checking them against your own expectation is the fastest way to confirm the inputs were read as you intended.

Can I rely on this for a production decision?

CMC(2:1) is the usual textile setting and tolerates lightness shifts twice as readily as chroma shifts. A negative margin means the batch fails. Treat the output as an engineering estimate that narrows the trial window, not as a substitute for the trial.

Scroll to Top