PVC Plastisol Coat Build & Fusion Dwell Calculator
Plastisol loses nothing to evaporation, so every micron of gap stays on the cloth. What it can lose is fusion, and an unfused film looks perfect until it peels.
Fused Weight per Coat
— g/m²
What one pass leaves on the cloth after fusion
Build & Fusion
- Wet Film per Coat
- — mm
- Wet Weight per Coat
- — g/m²
- Coats Required
- — no.
- Coating Weight Delivered
- — g/m²
- Finished Film Thickness
- — mm
- Fusion Dwell Adequacy
- — %
Fusion adequacy below 100% means the film gels but never fuses — it will look and feel finished while delaminating in service, and no amount of extra coating weight fixes it. Check fusion by solvent or tensile test on the finished cloth rather than by appearance.
Using this calculator
About the PVC Plastisol Coat Build & Fusion Dwell Calculator
The formula
This is the expression the tool evaluates. Every term is named underneath, with the unit it must be supplied in.
fusedWeightPerCoat = f( bladeGap, gapFactor, plastisolDensity, fusionShrinkage, targetFilmWeight, lineSpeed, ovenLength, fusionDwellRequired )Each input feeds the expression evaluated in the browser; the symbol table below names every term and its unit.
| Symbol | Stands for | Unit |
|---|---|---|
bladeGap | Blade Gap | mm |
gapFactor | Wet Film to Gap Factor | × |
plastisolDensity | Plastisol Density | g/cm³ |
fusionShrinkage | Fusion Shrinkage | % |
targetFilmWeight | Target Coating Weight | g/m² |
lineSpeed | Line Speed | m/min |
ovenLength | Fusion Oven Length | m |
fusionDwellRequired | Fusion Dwell Required | s |
fusedWeightPerCoat | Fused Weight per Coat | g/m² |
wetFilmPerCoat | Wet Film per Coat | mm |
wetWeightPerCoat | Wet Weight per Coat | g/m² |
coatsRequired | Coats Required | no. |
actualFilmWeight | Coating Weight Delivered | g/m² |
fusedThickness | Finished Film Thickness | mm |
fusionAdequacy | Fusion Dwell Adequacy | % |
How the result is derived
Step by step, from the values you type to the figure on screen.
- The 8 inputs are read from the form on every keystroke: Blade Gap, Wet Film to Gap Factor, Plastisol Density, Fusion Shrinkage, Target Coating Weight, Line Speed, Fusion Oven Length and Fusion Dwell Required.
- Each value is checked against the accepted range in the input table below. A value outside its range stops the calculation rather than producing a misleading figure — the results blank out and a message appears.
- The validated values are substituted into the expression above, which resolves Fused Weight per Coat together with every supporting figure in one pass — no value is carried over from a previous entry.
- The supporting outputs — Wet Film per Coat, Wet Weight per Coat, Coats Required, Coating Weight Delivered, Finished Film Thickness and Fusion Dwell Adequacy — come from the same pass, so they always describe the same case as the headline figure.
- Results are rounded for display only. The full-precision value is used throughout the chain, so reading a rounded intermediate figure back into the tool by hand can shift the last digit.
What each input means
Where to read each value on the floor, the unit it must be in, and the range the tool accepts.
| Input | Unit | Accepted range | Default | What it means |
|---|---|---|---|---|
| Blade Gap | mm | 0.02 to 5 mm | 0.35 | |
| Wet Film to Gap Factor | × | 0.4 to 1.2 × | 0.9 | |
| Plastisol Density | g/cm³ | 0.8 to 2 g/cm³ | 1.3 | |
| Fusion Shrinkage | % | 0 to 15 % | 3 | |
| Target Coating Weight | g/m² | 20 to 5000 g/m² | 500 | |
| Line Speed | m/min | 1 to 120 m/min | 20 | |
| Fusion Oven Length | m | 1 to 60 m | 12 | |
| Fusion Dwell Required | s | 1 to 300 s | 25 |
What the tool returns
The headline figure and every supporting value it is built from.
| Output | Unit | What it tells you |
|---|---|---|
| Fused Weight per Coat (headline result) | g/m² | What one pass leaves on the cloth after fusion |
| Wet Film per Coat | mm | |
| Wet Weight per Coat | g/m² | |
| Coats Required | no. | |
| Coating Weight Delivered | g/m² | |
| Finished Film Thickness | mm | |
| Fusion Dwell Adequacy | % |
Worked example
Given
- Blade Gap
- 0.35 mm
- Wet Film to Gap Factor
- 0.9 ×
- Plastisol Density
- 1.3 g/cm³
- Fusion Shrinkage
- 3 %
- Target Coating Weight
- 500 g/m²
- Line Speed
- 20 m/min
- Fusion Oven Length
- 12 m
- Fusion Dwell Required
- 25 s
The tool loads with this case already solved — the Fused Weight per Coat shown above is its answer. Change one value and the difference from this baseline is the sensitivity of the result to that variable.
How to use it
- Work through the input groups in order — Coating Head and Target & Oven. The defaults are a realistic case, so you can change one value at a time and watch what moves.
- There is no calculate button. Every figure recalculates as you type or drag, which is what makes this usable for a what-if sweep rather than a single answer.
- Read Fused Weight per Coat in the dark results panel — that is the headline figure, expressed in g/m².
- Check the supporting rows underneath (Wet Film per Coat, Wet Weight per Coat, Coats Required, Coating Weight Delivered, Finished Film Thickness and Fusion Dwell Adequacy) before acting on the headline — they are where an implausible input usually shows itself first.
- Reset to defaults returns every field to the reference case, which is the quickest way to check whether a surprising result came from the tool or from an input you had changed earlier.
Where this is used
- Process planning — establishing Fused Weight per Coat before a trial is booked, so machine time and material in Leather, Coated Fabrics & Tarpaulins are committed against a calculated figure rather than an estimate.
- Costing and quotation — Fused Weight per Coat is an input to the cost sheet, and quoting from a worked number rather than a remembered one is what keeps a margin intact.
- Troubleshooting — when the floor result drifts from plan, entering the measured values (starting with Blade Gap) shows how much of the gap in Fused Weight per Coat each variable explains.
- Teaching and study — the accepted ranges bracket normal Leather, Coated Fabrics & Tarpaulins practice, so moving one variable at a time shows the shape of the relationship rather than a single answer.
Assumptions and limits
- Fusion adequacy below 100% means the film gels but never fuses — it will look and feel finished while delaminating in service, and no amount of extra coating weight fixes it. Check fusion by solvent or tensile test on the finished cloth rather than by appearance.
- Every input is bounded to the range normal practice occupies (Blade Gap 0.02 to 5 mm, Wet Film to Gap Factor 0.4 to 1.2 × and Plastisol Density 0.8 to 2 g/cm³, and so on for the rest). Those bounds are guard rails against typing errors, not a claim that the formula fails one unit outside them.
- The calculation is deterministic: the same inputs always give the same result. It carries no allowance for machine condition, operator skill, ambient conditions or lot-to-lot material variation unless an input above explicitly represents one.
- Nothing is sent anywhere. The maths runs in your browser, so the numbers you type never leave the page.
Questions people ask
What do I need to know before using the PVC Plastisol Coat Build & Fusion Dwell Calculator?
Have these to hand: Blade Gap, Wet Film to Gap Factor, Plastisol Density, Fusion Shrinkage, Target Coating Weight, Line Speed, Fusion Oven Length and Fusion Dwell Required. With those entered, the tool returns Fused Weight per Coat immediately.
What exactly is Fused Weight per Coat?
What one pass leaves on the cloth after fusion. It is reported in g/m². It is derived from Blade Gap, Wet Film to Gap Factor, Plastisol Density, Fusion Shrinkage, Target Coating Weight, Line Speed, Fusion Oven Length and Fusion Dwell Required, and is the figure the rest of the Leather, Coated Fabrics & Tarpaulins calculation is built around.
Which units does this calculator expect?
Enter Blade Gap in mm, Wet Film to Gap Factor in ×, Plastisol Density in g/cm³, Fusion Shrinkage in %, Target Coating Weight in g/m², Line Speed in m/min, Fusion Oven Length in m and Fusion Dwell Required in s. Mixing unit systems is the most common cause of a result that looks an order of magnitude wrong — convert before typing, not after reading.
What are the other figures under the main result?
They are the intermediate quantities the calculation passes through: Wet Film per Coat, Wet Weight per Coat, Coats Required, Coating Weight Delivered, Finished Film Thickness and Fusion Dwell Adequacy. They are shown because a headline number nobody can trace is a number nobody trusts — checking them against your own expectation is the fastest way to confirm the inputs were read as you intended.
Can I rely on this for a production decision?
Fusion adequacy below 100% means the film gels but never fuses — it will look and feel finished while delaminating in service, and no amount of extra coating weight fixes it. Check fusion by solvent or tensile test on the finished cloth rather than by appearance. Treat the output as an engineering estimate that narrows the trial window, not as a substitute for the trial.