Jump to a calculator 671 tools
Lamination
Hot Melt PUR Lamination Dot Density & Application Rate
Every dot is a bond and a blocked pore. Dot lamination is the compromise, and coverage percentage is where you set it.
Adhesive Add-on
— g/m²
Reactive hot melt laid down as dots
Pattern & Supply
- Volume per Dot
- — mm³
- Surface Coverage
- — %
- Open Area Retained
- — %
- Adhesive Volume
- — cm³/m²
- Adhesive Consumption
- — kg/h
Dots are treated as cylinders, which over-states volume slightly against a real domed dot. Open area is a geometric ceiling on breathability, not a moisture vapour transmission rate — MVTR has to be measured on the finished laminate. Reactive PUR cures with ambient moisture: bond figures apply after full cure, not off the line.
Using this calculator
About the Hot Melt PUR Lamination Dot Density & Application Rate
The formula
This is the expression the tool evaluates. Every term is named underneath, with the unit it must be supplied in.
addOn = f( dotDiameter, dotHeight, dotsPerCm2, adhesiveDensity, lineSpeed, fabricWidth )Each input feeds the expression evaluated in the browser; the symbol table below names every term and its unit.
| Symbol | Stands for | Unit |
|---|---|---|
dotDiameter | Dot Diameter | mm |
dotHeight | Dot Height | mm |
dotsPerCm2 | Dot Density | dots/cm² |
adhesiveDensity | Adhesive Density | g/cm³ |
lineSpeed | Line Speed | m/min |
fabricWidth | Fabric Width | m |
addOn | Adhesive Add-on | g/m² |
dotVolume | Volume per Dot | mm³ |
coverage | Surface Coverage | % |
openArea | Open Area Retained | % |
volumePerSqM | Adhesive Volume | cm³/m² |
consumption | Adhesive Consumption | kg/h |
How the result is derived
Step by step, from the values you type to the figure on screen.
- The 6 inputs are read from the form on every keystroke: Dot Diameter, Dot Height, Dot Density, Adhesive Density, Line Speed and Fabric Width.
- Each value is checked against the accepted range in the input table below. A value outside its range stops the calculation rather than producing a misleading figure — the results blank out and a message appears.
- The validated values are substituted into the expression above, which resolves Adhesive Add-on together with every supporting figure in one pass — no value is carried over from a previous entry.
- The supporting outputs — Volume per Dot, Surface Coverage, Open Area Retained, Adhesive Volume and Adhesive Consumption — come from the same pass, so they always describe the same case as the headline figure.
- Results are rounded for display only. The full-precision value is used throughout the chain, so reading a rounded intermediate figure back into the tool by hand can shift the last digit.
What each input means
Where to read each value on the floor, the unit it must be in, and the range the tool accepts.
| Input | Unit | Accepted range | Default | What it means |
|---|---|---|---|---|
| Dot Diameter | mm | 0.05 to 5 mm | 0.4 | |
| Dot Height | mm | 0.01 to 3 mm | 0.15 | |
| Dot Density | dots/cm² | 1 to 400 dots/cm² | 40 | |
| Adhesive Density | g/cm³ | 0.5 to 2 g/cm³ | 1.15 | |
| Line Speed | m/min | 1 to 150 m/min | 20 | |
| Fabric Width | m | 0.2 to 5 m | 1.5 |
What the tool returns
The headline figure and every supporting value it is built from.
| Output | Unit | What it tells you |
|---|---|---|
| Adhesive Add-on (headline result) | g/m² | Reactive hot melt laid down as dots |
| Volume per Dot | mm³ | |
| Surface Coverage | % | |
| Open Area Retained | % | |
| Adhesive Volume | cm³/m² | |
| Adhesive Consumption | kg/h |
Worked example
Given
- Dot Diameter
- 0.4 mm
- Dot Height
- 0.15 mm
- Dot Density
- 40 dots/cm²
- Adhesive Density
- 1.15 g/cm³
- Line Speed
- 20 m/min
- Fabric Width
- 1.5 m
The tool loads with this case already solved — the Adhesive Add-on shown above is its answer. Change one value and the difference from this baseline is the sensitivity of the result to that variable.
How to use it
- Work through the input groups in order — Dot Pattern and Line. The defaults are a realistic case, so you can change one value at a time and watch what moves.
- There is no calculate button. Every figure recalculates as you type or drag, which is what makes this usable for a what-if sweep rather than a single answer.
- Read Adhesive Add-on in the dark results panel — that is the headline figure, expressed in g/m².
- Check the supporting rows underneath (Volume per Dot, Surface Coverage, Open Area Retained, Adhesive Volume and Adhesive Consumption) before acting on the headline — they are where an implausible input usually shows itself first.
- Reset to defaults returns every field to the reference case, which is the quickest way to check whether a surprising result came from the tool or from an input you had changed earlier.
Where this is used
- Process planning — establishing Adhesive Add-on before a trial is booked, so machine time and material in Coating, Lamination & Advanced Finishing are committed against a calculated figure rather than an estimate.
- Costing and quotation — Adhesive Add-on is an input to the cost sheet, and quoting from a worked number rather than a remembered one is what keeps a margin intact.
- Troubleshooting — when the floor result drifts from plan, entering the measured values (starting with Dot Diameter) shows how much of the gap in Adhesive Add-on each variable explains.
- Teaching and study — the accepted ranges bracket normal Coating, Lamination & Advanced Finishing practice, so moving one variable at a time shows the shape of the relationship rather than a single answer.
Assumptions and limits
- Dots are treated as cylinders, which over-states volume slightly against a real domed dot. Open area is a geometric ceiling on breathability, not a moisture vapour transmission rate — MVTR has to be measured on the finished laminate. Reactive PUR cures with ambient moisture: bond figures apply after full cure, not off the line.
- Every input is bounded to the range normal practice occupies (Dot Diameter 0.05 to 5 mm, Dot Height 0.01 to 3 mm and Dot Density 1 to 400 dots/cm², and so on for the rest). Those bounds are guard rails against typing errors, not a claim that the formula fails one unit outside them.
- The calculation is deterministic: the same inputs always give the same result. It carries no allowance for machine condition, operator skill, ambient conditions or lot-to-lot material variation unless an input above explicitly represents one.
- Nothing is sent anywhere. The maths runs in your browser, so the numbers you type never leave the page.
Questions people ask
What do I need to know before using the Hot Melt PUR Lamination Dot Density & Application Rate?
Have these to hand: Dot Diameter, Dot Height, Dot Density, Adhesive Density, Line Speed and Fabric Width. With those entered, the tool returns Adhesive Add-on immediately.
What exactly is Adhesive Add-on?
Reactive hot melt laid down as dots. It is reported in g/m². It is derived from Dot Diameter, Dot Height, Dot Density, Adhesive Density, Line Speed and Fabric Width, and is the figure the rest of the Coating, Lamination & Advanced Finishing calculation is built around.
Which units does this calculator expect?
Enter Dot Diameter in mm, Dot Height in mm, Dot Density in dots/cm², Adhesive Density in g/cm³, Line Speed in m/min and Fabric Width in m. Mixing unit systems is the most common cause of a result that looks an order of magnitude wrong — convert before typing, not after reading.
What are the other figures under the main result?
They are the intermediate quantities the calculation passes through: Volume per Dot, Surface Coverage, Open Area Retained, Adhesive Volume and Adhesive Consumption. They are shown because a headline number nobody can trace is a number nobody trusts — checking them against your own expectation is the fastest way to confirm the inputs were read as you intended.
Can I rely on this for a production decision?
Dots are treated as cylinders, which over-states volume slightly against a real domed dot. Open area is a geometric ceiling on breathability, not a moisture vapour transmission rate — MVTR has to be measured on the finished laminate. Reactive PUR cures with ambient moisture: bond figures apply after full cure, not off the line. Treat the output as an engineering estimate that narrows the trial window, not as a substitute for the trial.