Home » Calculators » Technical & Performance Textiles » Composites, Aerospace & Automotive Textiles » Woven Roving Thickness & Laminate Stack Planner
Jump to a calculator 671 tools

Composites

Woven Roving Thickness & Laminate Stack Planner

Put this calculator on your own site

Paste this where you want the calculator to appear. It works on any site — WordPress, Squarespace, Webflow, Ghost or plain HTML — and needs no JavaScript of yours. It carries a link back here, which is the only thing we ask for it.

See what it looks like

Ply thickness is not a property of the cloth — it is a property of the cloth and the volume fraction your process actually reaches.

Reinforcement Per ply
g/m²
g/cm³

E-glass 2.55, carbon 1.79, aramid 1.44.

%

Hand layup 30–40%, vacuum bag 45–55%, infusion 50–60%.

g/cm³
Laminate Target
mm

Cured Ply Thickness

— mm

At the achievable fibre volume fraction

Stack Plan

Plies Required
— no.
Thickness Delivered
— mm
Laminate Weight
— kg/m²
Resin Required
— kg/m²
Resin to Glass Ratio
— ×

Fibre volume fraction is the whole answer and it is a process property, not a material one — the same cloth hand-laid and infused differs by nearly half a ply in thickness. Resin demand here is what ends up in the laminate; add the consumables, feed lines and catch pot before ordering.

Using this calculator

About the Woven Roving Thickness & Laminate Stack Planner

The formula

This is the expression the tool evaluates. Every term is named underneath, with the unit it must be supplied in.

Cured ply thickness, mm
plyThickness = (fabricGsm / fibreDensity) / (targetFvf / 100) / 10000 x 10

The fibre volume per m² divided by the fibre volume fraction gives the ply volume per m²; spread over 10,000 cm² it gives the thickness.

Whole plies to reach at least the target
pliesRequired = ceil(targetThickness / plyThickness)
Resin left in each cured ply, g/m²
resinPerPly = (plyVolume - fibreVolume) x resinDensity

Assumes no voids. Add the resin lost to consumables, lines and the catch pot when ordering.

Symbols used above
SymbolStands forUnit
fabricGsmFabric Areal Weightg/m²
fibreDensityFibre Densityg/cm³
targetFvfAchievable Fibre Volume Fraction%
resinDensityResin Densityg/cm³
targetThicknessTarget Laminate Thicknessmm
plyThicknessCured Ply Thicknessmm
pliesRequiredPlies Requiredno.
actualThicknessThickness Deliveredmm
laminateArealWeightLaminate Weightkg/m²
resinDemandResin Requiredkg/m²
resinToGlassRatioResin to Glass Ratio×

How the result is derived

Step by step, from the values you type to the figure on screen.

  1. The 5 inputs are read from the form on every keystroke: Fabric Areal Weight, Fibre Density, Achievable Fibre Volume Fraction, Resin Density and Target Laminate Thickness.
  2. Each value is checked against the accepted range in the input table below. A value outside its range stops the calculation rather than producing a misleading figure — the results blank out and a message appears.
  3. The validated values are substituted into the expression above, which resolves Cured Ply Thickness together with every supporting figure in one pass — no value is carried over from a previous entry.
  4. The supporting outputs — Plies Required, Thickness Delivered, Laminate Weight, Resin Required and Resin to Glass Ratio — come from the same pass, so they always describe the same case as the headline figure.
  5. Results are rounded for display only. The full-precision value is used throughout the chain, so reading a rounded intermediate figure back into the tool by hand can shift the last digit.

What each input means

Where to read each value on the floor, the unit it must be in, and the range the tool accepts.

InputUnitAccepted rangeDefaultWhat it means
Fabric Areal Weightg/m²50 to 5000 g/m²800
Fibre Densityg/cm³1 to 3.5 g/cm³2.55E-glass 2.55, carbon 1.79, aramid 1.44.
Achievable Fibre Volume Fraction%15 to 75 %45Hand layup 30–40%, vacuum bag 45–55%, infusion 50–60%.
Resin Densityg/cm³0.8 to 2 g/cm³1.2
Target Laminate Thicknessmm0.2 to 200 mm12

What the tool returns

The headline figure and every supporting value it is built from.

OutputUnitWhat it tells you
Cured Ply Thickness (headline result)mmAt the achievable fibre volume fraction
Plies Requiredno.
Thickness Deliveredmm
Laminate Weightkg/m²
Resin Requiredkg/m²
Resin to Glass Ratio×

Worked example

Given

Fabric
800 g/m² E-glass (2.55 g/cm³)
Process
45% fibre volume, resin 1.2 g/cm³
Target
12 mm

Substituting

fibre volume = 800 / 2.55 = 313.7 cm3 per m2ply volume = 313.7 / 0.45 = 697.2 cm3; thickness = 0.697 mmplies = ceil(12 / 0.697) = ceil(17.2) = 18, giving 12.55 mmresin per ply = (697.2 - 313.7) x 1.2 = 460 g; x 18 = 8.28 kg/m2

Answer

Ply
0.697 mm
Plies
18 (12.55 mm)
Laminate
22.7 kg/m²
Resin
8.28 kg/m² (0.58 per kg glass)

Infused at 55% fibre volume the ply is thinner, 0.570 mm, so the same 12 mm needs 22 plies, and only 6.78 kg/m² of resin.

How to use it

  1. Work through the input groups in order — Reinforcement and Laminate. The defaults are a realistic case, so you can change one value at a time and watch what moves.
  2. There is no calculate button. Every figure recalculates as you type or drag, which is what makes this usable for a what-if sweep rather than a single answer.
  3. Read Cured Ply Thickness in the dark results panel — that is the headline figure, expressed in mm.
  4. Check the supporting rows underneath (Plies Required, Thickness Delivered, Laminate Weight, Resin Required and Resin to Glass Ratio) before acting on the headline — they are where an implausible input usually shows itself first.
  5. Reset to defaults returns every field to the reference case, which is the quickest way to check whether a surprising result came from the tool or from an input you had changed earlier.

Where this is used

  • Process planning — establishing Cured Ply Thickness before a trial is booked, so machine time and material in Composites, Aerospace & Automotive Textiles are committed against a calculated figure rather than an estimate.
  • Costing and quotation — Cured Ply Thickness is an input to the cost sheet, and quoting from a worked number rather than a remembered one is what keeps a margin intact.
  • Troubleshooting — when the floor result drifts from plan, entering the measured values (starting with Fabric Areal Weight) shows how much of the gap in Cured Ply Thickness each variable explains.
  • Teaching and study — the accepted ranges bracket normal Composites, Aerospace & Automotive Textiles practice, so moving one variable at a time shows the shape of the relationship rather than a single answer.

Reading the result

Typical bands and what each one is telling you.

ValueWhat it indicates
Higher fibre volume fractionThinner plies, so more plies for the same thickness, less resin and a stiffer, stronger laminate.
Delivered thickness well above targetThe last ply overshoots. A lighter fabric for the final ply brings the thickness closer.
Measured thickness above the planThe process reached a lower fibre volume than assumed, or the laminate has voids. Check consolidation and measure fibre content.

Assumptions and limits

  • Fibre volume fraction is the whole answer and it is a process property, not a material one — the same cloth hand-laid and infused differs by nearly half a ply in thickness. Resin demand here is what ends up in the laminate; add the consumables, feed lines and catch pot before ordering.
  • Every input is bounded to the range normal practice occupies (Fabric Areal Weight 50 to 5000 g/m², Fibre Density 1 to 3.5 g/cm³ and Achievable Fibre Volume Fraction 15 to 75 %, and so on for the rest). Those bounds are guard rails against typing errors, not a claim that the formula fails one unit outside them.
  • The calculation is deterministic: the same inputs always give the same result. It carries no allowance for machine condition, operator skill, ambient conditions or lot-to-lot material variation unless an input above explicitly represents one.
  • Nothing is sent anywhere. The maths runs in your browser, so the numbers you type never leave the page.

Standards and further reading

  • ISO 3374, reinforcement products, mats and fabrics: mass per unit area.
  • ISO 1172 and ASTM D2584, glass content of cured glass-reinforced plastics by ignition loss, to check the fibre volume reached.

Questions people ask

Why does the same cloth give different thicknesses?

Thickness depends on how much resin the process leaves in, not on the dry cloth. Hand layup leaves more resin than vacuum bagging or infusion.

How do I turn glass content by weight into fibre volume?

Vf = (Wf / fibre density) / (Wf / fibre density + (1 - Wf) / resin density), with Wf the glass weight fraction from an ignition-loss test.

Is resin to glass ratio the same as resin content?

No. A ratio of 0.58 means 0.58 kg of resin per kg of glass, which is a resin content of 0.58 / 1.58 = 37% by weight.

Scroll to Top

Follow on WhatsApp

Scan with your phone’s camera to open the channel, then tap Follow.

QR code for the WhatsApp channelOr open WhatsApp on this device