Gester Instruments GT-C15 is a fabric testing instrument, still in its builder’s current range. Its builder lists stroke length 25mm and weig ht 50 kg. Fabric testing instruments measure fabric properties such as tensile and tear strength, abrasion and pilling resistance, colour fastness, dimensional stability and air permeability.
Checked against the builder's page. On 2026-11-17 an automated check found every figure on this record on the builder's page, www.gester-instruments.com, and the page names this model. No editor has reviewed it; confirm against the source before sizing or ordering.
Fabric testingTesting and laboratoryIn the builder's current range
Key specifications
Specifications incomplete: 0 of 5 key figures recorded
- Test performed—
- Measuring range—
- Test stations / specimen holders—
- Test standards—
- Specimen size—
- Rubbing / friction stroke25 mm
Specification
| Parameter | Value |
|---|---|
| Stroke length | 25mm |
| Counter display | LCD |
| Power supply | AC 220V 50/60HZ |
| Weig ht | 50 kg |
| Press weights - 5pcs | Press weights - 5pcs |
| Micrometer calipers - 1pc | Micrometer calipers - 1pc |
| Flex Abrasion Test fixture - 1set | Flex Abrasion Test fixture - 1set |
| Surface Abrasion Test fixture -1 set | Surface Abrasion Test fixture -1 set |
| Power Line - 1pc | Edge & Fold Abrasion Test - 1set |
| Option accessories | Rubber membrane with Electrode |
Read from the builder's published page: www.gester-instruments.com, on 2026-11-16.
Check against the machine before you buy or budget on it. Builders publish a range and a configuration; the machine on your floor may be a different variant, may have been rebuilt, and may not carry the options these figures assume. This register records what the builder published, not what any individual machine does.
The record
- Read from
- www.gester-instruments.com,
- Last changed
Related machines
Also from Gester Instruments
Other machines of this kind: Fabric testing
Report incorrect information on this page
Tell us what is wrong and we will check it against the source. Reports are private, are never published, and go to an editor rather than into a comment thread.