Gester Instruments GT-C27 is a fabric testing instrument, still in its builder’s current range. Its builder lists nozzle pressure difference 4,000Pa, weight 93 kg and test time 10 ~ 15s. Fabric testing instruments measure fabric properties such as tensile and tear strength, abrasion and pilling resistance, colour fastness, dimensional stability and air permeability.
Fabric testingTesting and laboratoryIn the builder's current range
Key specifications
Specifications incomplete: 2 of 5 key figures recorded
- Test performedAutomatic ally
- Measuring range—
- Test stations / specimen holders—
- Test standardsGB/T 5453, GB/T 13764, ISO 9237, ISO 7231, ISO 5636, BS 5636, ASTM D737, DIN 53887, JISL1096, AFNORG 07-111, EDANA140.1, ISO 9073-15, NWSP 070.1
- Specimen size—
- Weight93 kg
Specification
| Parameter | Value |
|---|---|
| Standards | GB/T 5453, GB/T 13764, ISO 9237, ISO 7231, ISO 5636, BS 5636, ASTM D737, DIN 53887, JISL1096, AFNORG 07-111, EDANA140.1, ISO 9073-15, NWSP 070.1 |
| Test method | Automatic ally |
| Test time | 10 ~ 15s |
| Nozzle pressure difference | 4,000Pa |
| Specimen pressure difference | 1, 000Pa |
| Data port | RS232C |
| Permeability range | 0.1 ~ 12000mm/s |
| Measuring error | ≤±2 % |
| Measuring unit | mm/s, m3/m2/min, cm3/cm2/s, m3m2/h, L/dm2/min, L/m2/s, cfm |
| Testing area | 5cm 2, 20cm 2, 50cm 2, 100cm 2, Ф50mm (≈19.6cm 2 ), Ф70mm(≈38.3cm 2 ) |
| Power supply | AC 220V 50/60HZ, 2KW |
| Weight | 93 kg |
Read from the builder's published page: www.gester-instruments.com, on 2026-11-16.
Check against the machine before you buy or budget on it. Builders publish a range and a configuration; the machine on your floor may be a different variant, may have been rebuilt, and may not carry the options these figures assume. This register records what the builder published, not what any individual machine does.
The record
- Read from
- www.gester-instruments.com,
- Checked by
- Textile School,
- Last changed
Related machines
Also from Gester Instruments
Other machines of this kind: Fabric testing
Report incorrect information on this page
Tell us what is wrong and we will check it against the source. Reports are private, are never published, and go to an editor rather than into a comment thread.