Gester Instruments GT-D45B is a fabric testing instrument, still in its builder’s current range. Its builder lists range of speed 50-80rmp (adjustable), rubbing head diameter 16mm and counter range 0-999999. Fabric testing instruments measure fabric properties such as tensile and tear strength, abrasion and pilling resistance, colour fastness, dimensional stability and air permeability.
Fabric testingTesting and laboratoryIn the builder's current range
Key specifications
Specifications incomplete: 1 of 5 key figures recorded
- Test performed—
- Measuring range—
- Test stations / specimen holders—
- Test standardsAATCC 116, ISO 105 X16
- Specimen size—
- Weight15 kg
Specification
| Parameter | Value |
|---|---|
| Standards | AATCC 116, ISO 105 X16 |
| Drive Mode | Electronic |
| Test Loading | 1143g / 11.1±0.5N |
| Rubbing Head Diameter | 16mm |
| Sample Dize | ≥ 25×25mm |
| Crockmeter Cloth Size | 51×51mm |
| Range of Speed | 50-80rmp (adjustable) |
| Counter Range | 0-999999 |
| Power Supply | 1∮AC 220V 50/60HZ 100W |
| Dimensions (Lx Wx H) | 240×100×160mm |
| Weight | 15 kg |
Read from the builder's published page: www.gester-instruments.com, on 2026-11-16.
Check against the machine before you buy or budget on it. Builders publish a range and a configuration; the machine on your floor may be a different variant, may have been rebuilt, and may not carry the options these figures assume. This register records what the builder published, not what any individual machine does.
The record
- Read from
- www.gester-instruments.com,
- Checked by
- Textile School,
- Last changed
Related machines
Also from Gester Instruments
Other machines of this kind: Fabric testing
Report incorrect information on this page