Home » Machinery specifications » Hans Schmidt DN1 / DNW

Hans Schmidt DN1 / DNW

Checked by an editor

The DN series are robust mechanical hand-held tension meters with a large analogue dial and three V-grooved guide rollers. The DN1 measures the running tension of threads, fibres and wires in the textile, fibre and wire industries, in 12 ranges from 20–120 cN to 5–50 daN and for material up to 50000 tex. The DNW measures tension on pre-tensioned, fixed ropes up to 4 mm diameter, in 4 ranges up to 400 daN.

Yarn testingTesting and laboratoryIn the builder's current range

Specification

ParameterValueUnitComparable
DN1 measuring ranges availablevon 20 - 120 cN bis 5 - 50 daN
DN1 maximum tensionmax. 50daN
DN1 application range, textile industrybis zu 50000tex
DN1 application range, wire industrybis zu Ø 2.5 mm Cu
DN1-120 measuring range20 – 120cN
DN1-120 measuring head width65mm
DN1-200 measuring range20 – 200cN
DN1-200 measuring head width65mm
DN1-400 measuring range20 – 400cN
DN1-400 measuring head width65mm
DN1-1000 measuring range50 – 1000cN
DN1-1000 measuring head width65mm
DN1-2000 measuring range200 – 2000cN
DN1-2000 measuring head width116mm
DN1-3500 measuring range400 – 3500cN
DN1-3500 measuring head width116mm
DN1-5000 measuring range400 – 5000cN
DN1-5000 measuring head width116mm
DN1-8000 measuring range500 – 8000cN
DN1-8000 measuring head width116mm
DN1-10K measuring range2 – 10daN
DN1-10K measuring head width116mm
DN1-20K-L measuring range5 – 20daN
DN1-20K-L measuring head width216mm
DN1-30K-L measuring range5 – 30daN
DN1-30K-L measuring head width265mm
DN1-50K-L measuring range5 – 50daN
DN1-50K-L measuring head width265mm
DN1-20K-L to DN1-50K-L measuring head width with guide roller Code V1285mm
DN1 accuracy±1 % Vollausschlag (Full Scale) oder ±1 Skalenteilstrich
DN1 scale diameter54mm
Operating temperature range10 – 45ºC
Ambient humiditymax. 85% rel. humidity
Housing materialDie-cast aluminium
DN1 weight, net (gross), up to DN1-10Kca. 700 (1200)g0.7 kg
DN1 weight, net (gross), DN1-20K-L and higherca. 900 (2200)g
DN1 max. throughput speed, standard guide rollers2000m/min
DN1 max. throughput speed, guide rollers Code K3500m/min
DN1 max. throughput speed, guide rollers Code H5000m/min
DNW measuring ranges availablevon 10 - 100 daN bis 40 - 400 daN
DNW maximum rope diametermax. Ø 4mm
DNW-100K measuring range10 – 100daN
DNW-200K measuring range20 – 200daN
DNW-300K measuring range30 – 300daN
DNW-400K measuring range40 – 400daN
DNW measuring head width265mm
DNW accuracy±3 % Vollausschlag (Full Scale) oder ±1 Skalenteilstrich
DNW weight, net (gross)ca. 1100 (2400)g

Read from the builder's published page: www.hans-schmidt.com, on 2026-11-07.

Check against the machine before you buy or budget on it. Builders publish a range and a configuration; the machine on your floor may be a different variant, may have been rebuilt, and may not carry the options these figures assume. This register records what the builder published, not what any individual machine does.

The record

Read from
www.hans-schmidt.com,
Checked by
Textile School,
Last changed

All machinery specifications

Related machines

Report incorrect information on this page

Tell us what is wrong and we will check it against the source. Reports are private, are never published, and go to an editor rather than into a comment thread.

Scroll to Top

Follow on WhatsApp

Scan with your phone’s camera to open the channel, then tap Follow.

QR code for the WhatsApp channelOr open WhatsApp on this device