The ET series are hand-held electronic tension meters for measuring the running tension of threads, fibres and fine wires at narrow, hard-to-reach points, used in texturing, spinning and wire winding. The ETB and ETX use V-grooved guide rollers for thread speeds up to 2000 m/min; the ETPB and ETPX use fixed ceramic pins for thread speeds up to 6000 m/min and are for textile applications only. The ETB and ETPB are the basic units; the ETX and ETPX add a memory and a USB interface for data recording on a PC with the Tension Inspect 3 software.
Yarn testingTesting and laboratoryIn the builder's current range
Key specifications
Specifications incomplete: 1 of 5 key figures recorded
- Yarn test speed (evenness / hairiness)—
- Force capacity—
- Tensile (crosshead) speed—
- Yarn count range2 000 tex
- Test standards—
- Weight0.31 kg
- Make
Hans SchmidtGermanyhans-schmidt.com (the builder's website, opens in a new tab) All 17 machines from Hans Schmidt - Class
- Yarn testing
- Process stage
- Testing and laboratory
- Lifecycle
- In the builder's current range
- See it
- Exhibited at ITMA ASIA + CITME 2024, Shanghai, stand H8-A04 (as listed by the organiser)
Specification
| Parameter | Value | Unit | Comparable |
|---|---|---|---|
| Measuring ranges, ETB / ETX (5 ranges) | 0.3 - 100.0 cN bis 3 - 2000 cN | ||
| Measuring ranges, ETPB / ETPX (3 ranges) | 0.3 - 100.0 cN bis 2.0 - 500.0 cN | ||
| Measuring range, ETB-100 / ETX-100 | 0.3 – 100.0 | cN | |
| Measuring range, ETB-200 / ETX-200 | 2.0 – 200.0 | cN | |
| Measuring range, ETB-500 / ETX-500 | 2.0 – 500.0 | cN | |
| Measuring range, ETB-1000 / ETX-1000 | 3 – 1000 | cN | |
| Measuring range, ETB-2000 / ETX-2000 | 3 – 2000 | cN | |
| Measuring head width, ETB / ETX 100-500 types | 24 | mm | |
| Measuring head width, ETB / ETX 1000-2000 types | 38 | mm | |
| Measuring head width, ETPB / ETPX | 22 | mm | |
| Yarn count, ETB / ETX | bis zu 2000 | tex | |
| Yarn count, ETPB / ETPX | bis zu 500 | tex | |
| Thread speed, ETB / ETX guide rollers | 2000 | m/min | |
| Thread speed, ETPB / ETPX ceramic pins | 6000 | m/min | |
| Accuracy | ±1 % Full Scale (Messbereichsende) ±1 Digit (typisch ±0.5 % Full Scale) | ||
| Units | cN, g, N or lb, switchable | ||
| Overload protection | 200 % Full Scale | ||
| Measuring principle | Strain gauge, full bridge | ||
| Measuring roller deflection | 0.5 max. | mm | |
| Internal measuring frequency | ca. 1 | kHz | |
| Display | Colour TFT 128 x 160 | ||
| Temperature range | 10 – 45 | ºC | |
| Humidity | max. 85 | % rel. humidity | |
| Power supply | LiPo battery (approx. 20 h continuous operation, charging time approx. 3.5 h), USB plug-in power supply 100 – 240 V AC | ||
| Housing material | Aluminium | ||
| Weight, net (gross) | ca. 310 (1220) | g | 0.31 kg |
| Memory, ETX / ETPX | 60000 readings in 999 series |
Read from the builder's published page: www.hans-schmidt.com, on 2026-11-07.
Check against the machine before you buy or budget on it. Builders publish a range and a configuration; the machine on your floor may be a different variant, may have been rebuilt, and may not carry the options these figures assume. This register records what the builder published, not what any individual machine does.
The record
- Read from
- www.hans-schmidt.com,
- Checked by
- Textile School,
- Last changed
Related machines
Also from Hans Schmidt
Other machines of this kind: Yarn testing
Report incorrect information on this page
Tell us what is wrong and we will check it against the source. Reports are private, are never published, and go to an editor rather than into a comment thread.